VALOX™ FR PBT 365

SABIC® PC Resin

Valox FR PBT 365 Flame Retardant Grade

VALOX™ FR PBT 365 is an unreinforced, opaque PBT plastic offering superior chemical resistance, excellent dimensional stability, and a UL94V-0 flame rating at just 0.031″ for enhanced safety in thin-wall applications.

  • Character: Unreinforced, opaque, chemical resistance and dimensional stability
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Flame Rating: UL 94 V-0 (0.76 mm / 0.031″)
  • Heat Deflection Temp (HDT): 121°C @ 1.82 MPa
  • Tensile Strength at Yield: 41 MPa
  • Flexural Modulus: 2240 MPa
  • Izod Impact (Notched, 23°C): 640 J/m
  • Relative Temperature Index (RTI): 105°C
  • Specific Gravity: 1.33
  • Water Absorption (24hr): 0.14% (Very Low)

Application

  • Electrical Connectors & Sockets
  • Circuit Breakers and Switches
  • Automotive Sensor Housings
  • Appliance Components (e.g., Motor End Caps)
  • Industrial Control System Parts

Features & Benefits

Superior Flame Retardancy

This PBT VALOX 365 Resin achieves a UL94V-0 rating, ensuring your components meet strict safety standards and reduce fire risks in sensitive applications like electronics.

Reliable Mechanical Strength

It provides excellent tensile and flexural strength, leading to durable, warp-resistant parts that maintain their shape and integrity under mechanical stress.

Exceptional Thermal Stability

With a high Heat Deflection Temperature, components made from VALOX™ FR Resin 365 perform reliably in elevated temperature environments without deforming.

VALOX™ FR PBT resin natual color

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity