SABIC Lexan HFR1724 Flame Retardant
LEXAN™ Resin HFR1724 is a high-flow, flame-retardant polycarbonate designed for food contact applications. With UL94 V2 rating, excellent mold release, and global compliance potential, it’s ideal for transparent parts requiring safety, clarity, and easy processing.
- Character: 25 MFR, UL94 V2 rated.
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 58 MPa
- Tensile Modulus: 2,200 MPa
- Flexural Strength: 91 MPa
- Flexural Modulus: 2,200 MPa
- Elongation at Break: 110%
- Elongation at Yield: 6%
- Notched Izod Impact (23°C): 65 J/m
Impact Properties
- Unnotched Charpy Impact (23°C): No Break
- Notched Charpy Impact (23°C): 55 kJ/m²
Thermal Properties
- Heat Deflection Temp (1.8 MPa): 125°C
- Vicat Softening Temp (B/50): 142°C
- Coefficient of Thermal Expansion: 0.065 mm/m°C
Physical Properties
- Mold Shrinkage: 0.5 – 0.7%
- Specific Gravity: 1.2
- MFR (Melt Flow Rate): 25 g/10 min (300°C/1.2 kg)
Flame Performance
- UL94 Flame Rating: V2 (at 1.5 mm and 3.0 mm)
Processing Guidelines
- Recommended Melt Temperature: 280 – 310°C
- Mold Temperature: 80 – 110°C
- Drying Conditions: 2 – 4 hrs at 120°C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin HFR1724
LEXAN™ PC Resin HF4010SR
LEXAN™ PC Resin HF3510R
LEXAN™ PC Resin HFR1723
LEXAN™ PC Resin HF1840R
LEXAN™ PC Resin HF1140R
LEXAN™ PC Resin HF1140
LEXAN™ PC Resin HF1130R
LEXAN™ PC Resin HF1130
LEXAN™ PC Resin HF1110R
LEXAN™ PC Resin HF1110
LEXAN™ PC Resin GLX143
LEXAN™ PC Resin EX9332T
LEXAN™ PC Resin EX8681T
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
Advanced Manufacturing