SABIC Lexan IR1840 High Flow
LEXAN IR1840 resin is a high flow (MFR = 22 at 300℃/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. This material is food contact compliant in most jurisdictions.
- Character: high flow (MFR = 22 at 300℃/1.2kg), heat stabilized
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 60 MPa
- Flexural Modulus: 2,300 MPa
- Tensile Modulus: 2,300 MPa
- Elongation at Break: 120%
Impact Properties
- Notched Izod Impact (23°C): 65 kJ/m²
- Unnotched Izod Impact (23°C): No Break
Thermal Properties
- Vicat Softening Temperature (B/50): 148°C
- Heat Deflection Temperature (1.8 MPa): 130°C
Physical Properties
- Melt Flow Rate (300°C/1.2 kg): 22 g/10 min
- Density: 1.2 g/cm³
- Transparency: Transparent
Flame Performance
- UL94 Rating: V-2 @ 1.5 mm
- Glow Wire Ignition Temperature (GWIT): 775°C
Processing Guidelines
- Recommended Mold Temperature: 80–120°C
- Recommended Melt Temperature: 280–310°C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin IR1840
LEXAN™ PC Resin IR2210
LEXAN™ PC Resin IR2110
LEXAN™ PC Resin IR2040
LEXAN™ PC Resin IR1810
LEXAN™ PC Resin HFR1724
LEXAN™ PC Resin HF4010SR
LEXAN™ PC Resin HF3510R
LEXAN™ PC Resin HFR1723
LEXAN™ PC Resin HF1840R
LEXAN™ PC Resin HF1140R
LEXAN™ PC Resin HF1140
LEXAN™ PC Resin HF1130R
LEXAN™ PC Resin HF1130
LEXAN™ PC Resin HF1110R
LEXAN™ PC Resin HF1110
LEXAN™ PC Resin GLX143
LEXAN™ PC Resin EX9332T
Advanced Manufacturing