LEXAN™ PC Resin IR2110

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan IR2110 High Flow

LEXAN™ Resin IR2110 is a medium-high flow (MFR = 15 at 300℃/1.2kg), heat-stabilized polycarbonate resin, engineered for custom compounding. It does not contain UV stabilizer or mold release.

  • Character: MFR = 15 at 300℃/1.2kg), heat-stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength @ Yield: 62 MPa
  • Flexural Modulus: 2,300 MPa
  • Flexural Strength: 90 MPa
  • Tensile Modulus: 2,300 MPa

Impact Properties

  • Notched Izod Impact, 23°C: 75 J/m

Thermal Properties

  • Heat Deflection Temperature (HDT) @ 1.82 MPa: 127°C
  • Vicat Softening Point: 150°C

Physical Properties

  • Density: 1.20 g/cm³
  • Melt Flow Rate (300°C/1.2kg): 15 g/10 min

Flame Performance

  • UL 94 Rating: V-2 at 1.5 mm

Processing Guidelines

  • Processing Temperature: 280–310°C
  • Mold Temperature: 80–110°C

Features & Benefits

Optimized Flow for Easy Processing

With a medium-high melt flow rate of 15, LEXAN IR2110 ensures smooth, efficient molding—ideal for complex or high-volume parts.

Heat Stabilized for Thermal Durability

Engineered to perform under elevated temperatures, this grade offers reliable dimensional stability in thermally demanding applications.

Custom Compounding Flexibility

Free from UV stabilizers and mold release agents, LEXAN Resin IR2110 provides a clean base for tailored formulations and specialty blends.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top