Suke PC1003R Nylon 6 Resin Reinforced Grade Suke PA6 FG30B is a 30% glass-fiber reinforced nylon resin engineered for high strength, heat resistance (HDT 160–180°C), and UL94 V0 flame retardancy. Ideal for IT, electrical, and appliance industries, it ensures durability, safety, and precision in demanding applications. Key technical data (ISO) Download Application Suke PA6 FG30B

Suke Plastics PA6 FG30B Read More »

Suke Plastics PA6 YH800

Suke PA6 YH800 Nylon Injection Molding Plastic Granules Suke PA6 YH800 is a high-performance nylon 6 resin engineered for demanding industrial applications. With exceptional tensile strength (60.7 MPa), impact resistance (20.1 KJ/m²), and heat stability (HDT 71°C), these PA6 granules excel in injection molding grade processes, delivering durable, precision components for automotive, industrial, and electrical