PBT Resin

PBT Resin

VALOX™ FR PBT 865

Valox FR PBT 865 Flame Retardant Grade VALOX™ FR resin 865 is a 30% glass-filled, flame-retardant PBT/PET compound. It offers superior UL94 V-0 & 5VA ratings, excellent chemical resistance, and improved aesthetics, ideal for demanding electrical, appliance, and lighting components. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products Advanced Manufacturing

VALOX™ FR PBT 865 Read More »

VALOX™ FR PBT 771

Valox FR PBT 771 Flame Retardant Grade VALOX™ FR resin 771 is a 35% mineral/glass-filled, flame-retardant PBT grade. It offers superior chemical resistance, a UL94 V-0 rating at 0.75mm, and exceptional protection against electrical arcing, making it ideal for demanding electrical components. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products

VALOX™ FR PBT 771 Read More »

VALOX™ FR PBT 855

Valox FR PBT 855 Flame Retardant Grade VALOX™ FR resin 855 is a 15% glass-filled, flame-retardant PBT/PET compound. It offers a UL94 V-0 rating at 1.5mm, excellent chemical resistance, and superior aesthetics for demanding applications like appliances and lighting. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products Advanced Manufacturing

VALOX™ FR PBT 855 Read More »

VALOX™ FR PBT 855

Valox FR PBT 855 Flame Retardant Grade VALOX™ FR PBT 855 is a 15% glass-filled, flame-retardant PBT/PET compound. It offers a UL94 V-0 rating at 1.5mm, excellent chemical resistance, and superior aesthetics for demanding applications like appliances and lighting. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products Advanced Manufacturing

VALOX™ FR PBT 855 Read More »

VALOX™ FR PBT 780

Valox FR PBT 780 Flame Retardant Grade VALOX™ FR resin 780 is a flame-retardant PBT/PET plastic compound, reinforced with minerals and glass fibers. It offers superior electrical insulation, high mechanical strength, and a reduced blooming effect, making it a reliable and versatile choice for demanding electronic and electrical components. Key technical data Download Application Features

VALOX™ FR PBT 780 Read More »

VALOX™ FR PBT 553U

Valox FR PBT 553U Flame Retardant Grade VALOX™ FR resin 553U is a 30% glass-filled, flame-retardant PBT/PC blend. It offers superior strength, minimal warpage, and a UL94 V-0 rating at 0.86mm, ideal for demanding electrical and structural components. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products Advanced Manufacturing

VALOX™ FR PBT 553U Read More »

VALOX™ FR PBT 457

Valox FR PBT 457 Flame Retardant Grade VALOX 457 Polybutylene Terephthalate (PBT) resin is a 6.5% glass fiber reinforced, flame retardant grade. It offers a UL 94 V-0 & 5VA rating, high-performance choice for demanding electrical components. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products Advanced Manufacturing

VALOX™ FR PBT 457 Read More »

VALOX™ FR PBT 420SE0

Valox FR PBT 420SE0 Flame Retardant Grade VALOX™ FR Resin 420SE0 is a 30% glass-filled, flame-retardant PBT grade. It offers excellent chemical resistance and is UL94 V-0 (0.71mm) & 5VA (2.0mm) rated, making it ideal for demanding electrical components. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products Advanced Manufacturing

VALOX™ FR PBT 420SE0 Read More »

VALOX™ FR PBT 553

Valox FR PBT 553 Flame Retardant Grade VALOX™ FR Resin 553 is a 30% glass-filled, flame-retardant PBT/PC alloy. It offers excellent chemical resistance, superior dimensional stability with low warpage, and top-tier UL94 V-0 & 5VA flammability ratings for demanding applications. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products Advanced Manufacturing

VALOX™ FR PBT 553 Read More »

VALOX™ FR PBT 365

Valox FR PBT 365 Flame Retardant Grade VALOX™ FR PBT 365 is an unreinforced, opaque PBT plastic offering superior chemical resistance, excellent dimensional stability, and a UL94V-0 flame rating at just 0.031″ for enhanced safety in thin-wall applications. Key technical data Download Application Features & Benefits Related Valox™ FR PBT Products Advanced Manufacturing

VALOX™ FR PBT 365 Read More »