Kibisan® PN-107 L125FG Low Residual Monomer Grade SAN
Kibisan PN-107 L125FG is a premium SAN resin made for high performance. It has low monomer residue, meeting EU 10/2011 and GB4806 standards, ensuring safety for food applications. With its high flowability, strength, and excellent transparency, this material is ideal for food containers, sealed cans, and cosmetic boxes. It’s easy to process and delivers reliable durability.
- Manufacturer: CHIMEI
- Application: Food containers, sealed cans, cosmetic boxes
- Character: Low monomer residue, High flowability, high transparency

Download
Access essential product documentation including technical datasheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.

Kibisan® PN-107 L125FG Datasheet
| Low Residual Monomer SAN KIBISAN® PN-107 L125FG | ||||
| Product Description: High clarity | ||||
| Properties | ISO Test Method | Test Condition | Unit | PN-107_L125FG |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 58 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.06 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 65 |
| 50 mm/min, break | MPa | 65 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 3 |
| Flexural Strength | 178 | 2 mm/min | MPa | 89 |
| Flexural Modulus | 178 | 2 mm/min | GPa | 2.6 |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 2 |
| -30℃, Notched | KJ/m2 | – | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 2 |
| -30℃, Notched | KJ/m2 | – | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 104 |
| 50℃/hr;5KG | ℃ | 101 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 88 |
| 1.8MPa, annealed | ℃ | 99 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 3.6~3.8*10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB |
| Mold Shrinkage | 294-4 | – | % | 0.2~0.7 |
| Symbol | 1043 | – | – | >SAN< |
| March 11, 2024 | ||||
Kibisan® PN-107 L125FG UL Product iQ
| KIBISAN® PN-107 L125 FG UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Styrene Acrylonitrile (SAN) “KIBISAN”, furnished as pellets |
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 5 | |
| 3.0 mm | PLC 4 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 1 | |
| 3.0 mm | PLC 1 | |
| Comparative Tracking Index (CTI) | PLC 2 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 1 | |
| High Voltage, Low Current Arc Resistance | PLC 6 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 50 °C | |
| 3.0 mm | 50 °C | |