Chimei Polylac ABS Resin PA-757H

Polylac® PA-757H High Flow Grade Medium Strength ABS

POLYLAC PA-757H by Chimei is a high-flow, high-impact ABS resin engineered for demanding applications. Combining exceptional moldability (30 ml/10 min MFI) with robust impact resistance (25 KJ/m²) and a glossy finish, it’s ideal for household appliances, motorcycle parts, and thin-walled components. Trusted for performance and reliability.

  • Manufacturer: Chimei
  • Character: High flowability, medium strength
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 30 ml/10 min (220°C, 10kg)
  • Impact Strength: 25 KJ/m² (23°C) / 12 KJ/m² (-30°C)
  • Heat Resistance: Vicat Softening Temp 105°C; HDT 83°C (1.8MPa)
  • Flammability: UL94 HB (1.5mm)
  • Mold Shrinkage: 0.4–0.7%

High Flow & Impact Balance

POLYLAC PA-757H delivers unmatched melt flow (30 ml/10 min) and Izod impact strength (25 KJ/m²), enabling fast production of thin-walled parts without sacrificing durability. Perfect for reducing cycle times in appliances like vacuum cleaner housings.

Premium Surface Gloss

With its high-gloss finish, ABS PA 757H eliminates the need for secondary painting, cutting costs for visible components like motorcycle fairings or sleek refrigerator panels.

Reliable Thermal Stability

PA-757H withstands heat up to 105°C (Vicat), ensuring parts like hair dryer nozzles or automotive trim retain shape and strength even under prolonged thermal stress.

Chimei Polylac PA-757H ABS

Application

  • Household Appliances: in thin-walled blender jars or coffee maker housings.
  • Motorcycle Parts: from glossy helmet shells to durable side panels.
  • Large/Thin-Wall Components: TV bezels or laptop casings.
Chimei Polylac PA-757H Application

Chimei Polylac® PA-757H Datasheet

General ABS POLYLAC® PA-757H
Product Description: Better balance in high flow and high impact, High gloss
PropertiesISO Test MethodTest ConditionUnitPA-757H
Melt Flow Index1133220℃×10KGml/10 min30
Mass Density118323  ℃g/cm31.04
Tensile Strength52750 mm/min, yieldMPa39
50 mm/min, breakMPa31
Tensile Elongation52750 mm/min%45
Flexural Strength1782 mm/minMPa61
Flexural Modulus2 mm/minGPa2
Izod Impact Strength180/1A23℃, NotchedKJ/m225
-30℃, NotchedKJ/m212
Charpy Impact Strength17923℃, NotchedKJ/m226
-30℃, NotchedKJ/m213
Vicat Softening Temp.30650℃/hr;1KG105
50℃/hr;5KG97
Heat Distortion Temp.75/A1.8MPa, unannealed83
1.8MPa, annealed98
Coefficient of Linear113598.6 x 10-5
Thermal Expansion
Flammability294-4UL-941.5mm HB
Mold Shrinkage1043%0.4~0.7
Symbol>ABS<

Related Polylac® ABS Plastics

No post found!

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top