Key technical data
- Tensile Strength (Yield): 90 MPa
- Flexural Modulus: 4250 MPa
- Izod Impact (Notched): 8 kJ/m²
- Heat Deflection Temp (HDT/A @1.8 MPa): 123 °C
- Vicat Softening Temperature (B/120): 136 °C
- Relative Temperature Index (RTI): 60 °C
- Physical & Processing Properties
- Melt Volume Rate (260°C/5kg): 33 cm³/10 min
- Mold Shrinkage: 0.3 – 0.5 %
- Density: 1.22 g/cm³
- Volume Resistivity: >1E+15 Ω·cm
Application
- Automotive Interior & Exterior Parts
- Electrical Enclosures & Housings
- Consumer Electronics Housings
- Industrial Components