TAIRIREX® GP5350 GPPS Resin General Grade

TAIRIREX GP5350 is a high-heat-resistant general-purpose polystyrene (GPPS) resin in pellet form, designed for demanding applications requiring durability, clarity, and thermal stability. With superior heat deflection and mechanical performance, it’s ideal for kitchenware, lighting, and consumer goods where reliability under stress matters.

  • Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
  • Character: High heat resistance
  • Application: Kitchen ware, Lamp covers, Decorated sheets, Toys
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 4.5 g/10min (200°C, 5kg)
  • Impact Strength: 1.6 kJ/m² (IZOD, unnotched) | 10.8 kJ/m² (Charpy)
  • Tensile Strength: 44 MPa | Flexural Strength: 76 MPa
  • Heat Resistance: Vicat Softening Point 100°C | Heat Deflection Temp. 95°C
  • Safety: UL 94 HB rated (1.5–1.7 mm thickness)
  • Residual Monomer: ≤700 ppm

Features & Benefits

Exceptional Heat Resistance

WiTAIRIREX GP5350 withstands temperatures up to 100°C (Vicat Softening Point), ensuring stability in hot environments—perfect for dishwasher-safe kitchenware or heat-exposed lamp covers.th a

High Mechanical Strength

With 44 MPa tensile strength and 76 MPa flexural strength, this TAIRIREX PS resin resists deformation under load, ideal for durable toys and structural components.

Easy Processing & Safety

The resin’s balanced melt flow (4.5 g/10min) simplifies molding, while its UL 94 HB flammability rating ensures safety in electrical components and decorative sheets.

Formosa Plastics TAIRIREX GP535N GPPS Resin

Application

Kitchenware

Heat-resistant utensils, containers, and cutlery.

Lamp Covers

Durable housings for LED and fluorescent lighting.

Decorated Sheets

Scratch-resistant surfaces for signage and displays.

Toys

Sturdy, safe components for children’s products.

Formosa Plastics TAIRIREX GP5250 application

Get to Know Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top