Suke Plastics PA6 YH800

Suke Modified plastics Nylon PA6 YH800

Suke PA6 YH800 Nylon Injection Molding Plastic Granules

Suke PA6 YH800 is a high-performance nylon 6 resin engineered for demanding industrial applications. With exceptional tensile strength (60.7 MPa), impact resistance (20.1 KJ/m²), and heat stability (HDT 71°C), these PA6 granules excel in injection molding grade processes, delivering durable, precision components for automotive, industrial, and electrical systems.

  • Manufacturer: Suke Plastics
  • Character: with Good Mechanical Properties and Recyclability for Pips and Bearings, fishing net.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Tensile Strength: 60.7 MPa
  • Impact Resistance: 20.1 KJ/m²
  • Heat Distortion Temp: 71°C
  • Moisture Content: <0.07%
  • Molding Shrinkage: 0.93%
  • Flexural Modulus: 2087 MPa

High Strength, Lightweight Design

Boasting 60.7 MPa tensile strength and a low density (1.156 g/cm³), YH800 Nylon PA6 reduces part weight without sacrificing structural integrity—ideal for automotive brackets or machinery housings.

Toughness Under Stress

With 20.1 KJ/m² notched impact resistance, these PA6 granules withstand sudden shocks, perfect for gears, bearings, or sports equipment prone to high-impact loads.

Heat & Moisture Resistance

Stable up to 71°C (HDT) and minimal moisture absorption (<0.07%), YH800 maintains performance in humid or high-temperature environments, like under-hood automotive parts.

Suke Plastics PA6 YH800

Application

  • Industrial Bearings & Pipes
  • Recyclable Automotive Components
  • Electrical Insulators
Suke PA6 YH800 Application

Suke PA6 YH800 Datasheet

General Grade Suke PA6 YH800 Data Sheet
Product Description: transparency
Physical PropertiesTest StandardUnitsTypical Value
DensityGB/T1033-1986g/cm³1.156
RSVFZ-T51004-20112.80±0.05
ExtractablesFZ-T51004-2011%<0.03
MoistureContentFZ-T51004-2011%<0.07
TensileStrengthGB1040-92MPa60.7
ElongationGB1040-92%48.1
BendingStrengthGB9341-88MPa86.6
FlexuralModulusGB9341-88MPa2087
HardnessGB9342-88R72.2
NotchedImpactStrengthGB/T1043-93KJ/㎡20.1
MoldingShrinkage%0.93
MeltingPoint215-220
HeatDistortionTemperatureGB1843-7971
PermittivityGB/T1409-20060.65

Get to Know Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top