FCFC Formosa TAIRIREX® GP5250

Formosa Plastics TAIRIREX GP5250

TAIRIREX® GP5250 General Grade Injection Molding

TAIRIREX GP5250 is a top-notch GPPS resin from FCFC Taiwan, perfect for injection molding. It flows easily for simple shaping and shines with great clarity for see-through containers and housewares. It resists static and chemicals well, and it’s safe for medical use with USP Class VI approval. Its key stats include a melt flow index of 6.7 g/10min and tensile strength of 41 MPa.

  • Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
  • Character: Injection molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Melt Flow Index: 6.7 g/10min (200°C, 5kg)
  • Tensile Strength: 41 MPa
  • Flexural Strength: 70 MPa
  • Izod Impact Strength: 1.6 kJ/m² (unnotched)
  • Vicat Softening Point: 95°C
  • Heat Deflection Temperature: 91°C (1.8 MPa)
  • Flammability: UL-94 HB rated

Features & Benefits

Easy to Process

With a melt flow index of 6.7 g/10min, GP5250 flows smoothly during injection molding, reducing cycle times and boosting production efficiency. This ensures faster turnaround and lower manufacturing costs for your operations.

Crystal Clear Transparency

The exceptional transparency of gpps gp5250 makes it perfect for applications requiring visual appeal, such as cosmetic cases and lamp decorations. Its clarity elevates product aesthetics, helping your brand stand out.

Strong and Durable

Featuring a tensile strength of 41 MPa and flexural strength of 70 MPa, GP5250 delivers robust, long-lasting products that withstand daily wear.

Formosa Plastics TAIRIREX GP5250 GPPS Resin

Application

  • Food Containers: Produces safe, clear, and durable containers that keep food fresh and visually appealing.
  • Stationery: Creates functional, transparent pen barrels, rulers, and other items with lasting quality.
  • Toys: Crafts strong, safe, and vibrant toys that meet child safety standards and delight users.
  • Clothing Hangers: Delivers sturdy hangers capable of supporting heavy garments without breaking.
  • Lamp Decoration: Offers beautiful light diffusion through transparent, elegant components.
  • Media Cases: Provides clear, protective cases for CDs, DVDs, and other media formats.
  • Cosmetic Cases: Enhances brand appeal with premium, crystal-clear packaging that showcases products.
Formosa Plastics TAIRIREX GP5250 application

Tairirex® GP5250 Datasheet

General purpose grade FCFC TAIRIREX® GP5250 Data Sheet
Product Description: Injection molding
PropertyUnitTest MethodTest ConditionModel GP5250
Melt Flow Indexg/10minISO 1133200℃ × 5kg 49N6.7
IZOD Impact StrengthkJ/m²ISO 18023℃, 4mm, Unnotched1.6
Charpy Impact StrengthkJ/m²ISO 17923℃, 4mm GPPS has no notch, HIPS has a notch7.4
Tensile StrengthMpaISO 52723℃, 20mm/min41
Tensile ModulusMpaISO 52723℃, 1mm/min3300
Tensile Elongation%ISO 52723℃, 20mm/min3
Flexural StrengthMpaISO 17823℃, 2mm/min70
Flexural ModulusMpaISO 17823℃, 2mm/min3200
Vicat Softening PointISO 306Annealed 80℃*2hr, 4mm,10N 50℃/h95
Heat Deflection TemperatureISO 75/AAnnealed 80℃*2hr,120℃/h,1.8Mpa 4mm91
CombustibilityUL-94File No. E162823HB 1.5 ~ 1.7 mm

Tairirex® GP5250 UL Product iQ

TAIRIREX® GP525# UL Product iQ
File Number: E162823Polystyrene (PS), pellets
(H) – Replace by one digital 0-9 or one alphabet H, unconcerned with formula or constituent changed
FlammabilityValueTest Method
Flame Rating
0.8 mm, ALLHBUL 94
1.0 mm, ALLHBUL 94
1.5 mm, ALLHBUL 94
3.0 mm, ALLHBUL 94
3.0 mm, ALLHB40IEC 60695-11-10, -20
0.8 mm, ALLHB75IEC 60695-11-10, -20
1.0 mm, ALLHB75IEC 60695-11-10, -20
1.5 mm, ALLHB75IEC 60695-11-10, -20
ElectricalValueTest Method
Hot-wire Ignition (HWI)UL 746
0.8 mmPLC 4
1.0 mmPLC 4
1.5 mmPLC 3
High Amp Arc Ignition (HAI)UL 746
0.8 mmPLC 3
1.0 mmPLC 3
1.5 mmPLC 3
Comparative Tracking Index (CTI)PLC 2UL 746
High Voltage Arc Tracking Rate (HVTR)PLC 1UL 746
Arc ResistancePLC 6ASTM D495
ThermalValueTest Method
RTI ElecUL 746
0.8 mm50.0°C
1.0 mm50.0°C
1.5 mm50.0°C
3.0 mm50.0°C
RTI ImpUL 746
0.8 mm50.0°C
1.0 mm50.0°C
1.5 mm50.0°C
3.0 mm50.0°C
RTI StrUL 746
0.8 mm50.0°C
1.0 mm50.0°C
1.5 mm50.0°C
3.0 mm50.0°C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top