Suke Plastics PA6 FG30B

Suke Modified plastics Nylon PA6 FG30B

Suke PC1003R Nylon 6 Resin Reinforced Grade

Suke PA6 FG30B is a 30% glass-fiber reinforced nylon resin engineered for high strength, heat resistance (HDT 160–180°C), and UL94 V0 flame retardancy. Ideal for IT, electrical, and appliance industries, it ensures durability, safety, and precision in demanding applications.

  • Manufacturer: Suke Plastics
  • Character: Glass-fiber Reinforced Grade
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Heat Resistance: 160–180°C (HDT @1.82MPa)
  • Mechanical Performance: Tensile Strength 90±5 MPa | Impact Strength 10 KJ/m²
  • Flammability: UL94 V0 (3.0mm thickness)
  • Electrical Insulation: Volume Resistivity 10¹⁵ Ω·cm
  • Molding Precision: Low shrinkage (1.1–1.3%) for tight-tolerance parts

High-Temperature Stability

With a heat distortion temperature of 160–180°C, PA6 FG30B resin withstands extreme thermal stress, preventing warping in components like power tool housings or automotive connectors.

Exceptional Mechanical Strength

Tensile strength of 90 MPa and rigid glass fiber reinforcement ensure structural integrity for gears, brackets, and industrial housings under heavy loads or repetitive stress.

Flame-Retardant Safety

UL94 V0 certification minimizes fire risks, making it ideal for circuit breakers, electrical enclosures, and smart device components requiring compliance with strict safety standards.

Suke Plastics PA6 FG30B

Application

  • IT & Communications: Server connectors, 5G router housings.
  • Electrical Appliances: Circuit breakers, switchgear components.
  • Household Appliances: Durable coffee machine gears, vacuum cleaner structural parts.
  • Industrial Electrical: Motor housings, relay insulators.

Suke PA6 FG30B Datasheet

General Grade Suke PA6 FG30B Data Sheet
Product Description: Glass-fiber Reinforced Grade
Physical PropertiesTest StandardTest conditionsUnitsTypical Value
Tensile StrengthsISO 52750mm/minMPa90±5
Elongation at Break FlexuralISO 52750mm/min%7.5±0.5
Pencil HardnessISO 203923℃,750gR109 
Notched Impact StrengthsISO 17923℃KJ/m²10.0±0.5
Linear Mold ShrinkageISO 29423℃%1.1-1.3
DensityISO 118323℃,10gg/cm³1.25±0.05
Heat Distortion TemperatureISO 751.82MPa160-180
FlammabilityUL 943.0mm    ClassV0
Volume ResistivityISO 143093.0mm Ω ·cm1015 
Processing conditionsRANGE
Drying Temperature100-140 ℃
Drying Time2.0-4.0 H
Cylinder Temperature240-260 ℃
Mold Temperature80-100 ℃

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top