Chimei Polylac® PA-758 L125 MABS

Chimei Polylac PA-758 L125 MABS Resin

POLYLAC® PA-758 L125 Transparent Grade Blue Tint MABS Resin

POLYLAC PA-758 L125 is a transparent MABS resin with a distinctive blue tint, combining high flowability for intricate molds and durability for demanding applications. Ideal for appliances, electronics, and industrial components requiring clarity, impact resistance, and ease of processing.

  • Character: Transparency with blue tint, chemical resistance, comply with Bio-compatibility test (ISO10993)
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Melt Flow Index: 3 ml/10 min
  • Tensile Strength: 42 MPa (yield)
  • Izod Impact (23°C): 14 KJ/m²
  • Vicat Softening Temp.: 104°C
  • Flammability Rating: UL 94 HB
  • Mold Shrinkage: 0.3–0.7%

Superior Flowability for Complex Designs

With a melt flow index of 3 ml/10 min (200°C/5KG), PA-758 L125 fills thin-walled or intricate molds effortlessly, reducing cycle times and production costs. Perfect for detailed components like 3C product casings.

High Impact Resistance & Strength

It boasts 14 KJ/m² Izod impact strength (23°C) and 42 MPa tensile strength, ensuring durability in high-stress environments. Ideal for washing machine covers and vacuum cleaner casings prone to drops or vibrations.(0.3-0.7%), ensuring consistent part quality and dimensional stability.

Heat & Chemical Stability

A Vicat softening temperature of 104°C (1KG) and UL 94 HB flammability rating make it reliable for heat-resistant parts like air conditioning panels or components exposed to household chemicals.

Polylac PA-758 L125 MABS Resin

Applications

  • Air conditioning panels: Heat-resistant, scratch-proof surfaces.
  • Washing machine covers: Impact-resistant, chemical-resistant housings.
  • Vacuum cleaner casings: Lightweight yet durable for daily wear.
  • 3C product casings (computers, cameras, communication devices): Sleek transparency for aesthetic tech parts.
  • Household appliances: Microwave buttons, blender components.
  • Stationery: Transparent rulers, ergonomic tool casings.
Chimei Polylac PA-758 L125 application

Polylac® PA-758_L125 Datasheet

Transparent MABS POLYLAC®  PA-758_L125
Product Description: Transparent blue
PropertiesISO Test MethodTest ConditionUnitPA-758_L125
Melt Flow Index1133 200℃×5KGml/10 min3.0 
Mass Density1183 23 ℃g/cm31.08 
Tensile Strength527 50 mm/min, yieldMPa42 
50 mm/min, breakMPa33 
Tensile Elongation527 50 mm/min%35 
Flexural Strength178 2 mm/minMPa57 
Flexural Modulus2 mm/minGPa1.9 
Izod Impact Strength180/1A23℃, NotchedKJ/m214 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m214 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG104 
50℃/hr;5KG96 
Heat Distortion Temp.75/A1.8MPa, unannealed77 
1.8MPa, annealed97 
Coefficient of Linear
Thermal Expansion
11359 9.0 x 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.3 ~ 0.7
Symbol1043 >MABS<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test

Polylac® PA-758_L125 UL Product iQ

POLYLAC® PA-758 UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
3.0 mmPLC 3
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 3
3.0 mmPLC 3
Comparative Tracking Index (CTI)PLC 0UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 0
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
Report Date: 1983-06-23

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top