Key technical data (ISO)

  • Melt Flow Index: 2.6 ml/10 min (200°C, 5KG)
  • Izod Impact Strength: 13 KJ/m² (23°C), 8 KJ/m² (-30°C)
  • Vicat Softening Temp: 100°C (1KG load)
  • Flammability: UL94 HB (1.5mm)
  • Mold Shrinkage: 0.4–0.7%

Superior Impact Resistance

POLYREX PH-88S delivers 13 KJ/m² Izod impact strength (23°C) and retains 8 KJ/m² at -30°C, ensuring durability in cold environments. Perfect for freezer-safe packaging or outdoor equipment.

Heat & Dimensional Stability

With a Vicat softening point of 100°C and low mold shrinkage (0.4–0.7%), this High Impact HIPS resists warping under heat, making it reliable for appliances like washing machine inner casings.

Easy Processing & Safety Compliance

A balanced melt flow index (2.6 ml/10 min) ensures smooth extrusion. HB flammability rating and FDA-compliant properties make it safe for food packaging and disposable cups.

Chimei POLYREX PH-88S

Applications

  • Disposable Cups & Food Packaging
  • Washing Machine Inner Casings
  • Spools & Profile Extrusions
  • Outdoor Equipment
Chimei POLYREX PH-88S application

Polyrex® PH-88S Datasheet

Extrusion HIPS POLYREX® PH-88S
Product Description: Extrusion
PropertiesISO Test MethodTest ConditionUnitPH-88S
Melt Flow Index1133 200℃×5KGml/10 min2.6 
Mass Density1183 23 ℃g/cm31.05 
Tensile Strength527 50 mm/min, yieldMPa28 
50 mm/min, breakMPa24 
Tensile Elongation527 50 mm/min%55 
Flexural Strength178 2 mm/minMPa34 
Flexural Modulus2 mm/minGPa1.4 
Izod Impact Strength180/1A23℃, NotchedKJ/m213 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m214 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG100 
50℃/hr;5KG89 
Heat Distortion Temp.75/A1.8MPa, unannealed77 
1.8MPa, annealed94 
Coefficient of Linear
Thermal Expansion
11359 4~6×10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.7
Symbol1043 >PS-HI<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users
should confirm results by their own test

Polyrex® PH-88S UL Product iQ

ACRYREX® PH-88S | UL Product iQ
File Number: E56070Yellow Card™Polystyrene (PS) “POLYREX”, furnished as pellets or powder
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 3
3.0 mmPLC 3
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 0
3.0 mmPLC 0
High Voltage Arc Tracking Rate (HVTR)PLC 3
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top