Chimei POLYREX® PH-888G HIPS

Chimei POLYREX® PS Resin PH-888G

Polyrex® PH-888G HIPS Extrusion Grade High Gloss


Chimei POLYREX PH-888G is a high-impact, high-gloss HIPS resin engineered for durability and aesthetics. The material solves pain points in manufacturing—combining toughness, heat stability, and a ready-to-use finish, perfect for appliances, electronics, and industrial components. Trusted by engineers for demanding applications.

  • Character: Heat and impact resistant, high gloss
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Impact Strength: 11 KJ/m² (23°C) | 5 KJ/m² (-30°C)
  • Heat Resistance: Vicat Softening Point 102°C | Heat Distortion Temp 79–95°C
  • Mechanical Strength: Tensile Strength 35 MPa | Flexural Strength 48 MPa
  • Safety Compliance: UL94 HB flammability rating (1.5mm)
  • Ease of Molding: Low shrinkage (0.4–0.7%)

Superior Impact Resistance

POLYREX PH-888G delivers 11 KJ/m² Izod impact strength (23°C), ensuring components withstand drops, vibrations, and rough handling. Perfect for monitor housings or fan blades requiring long-term durability.

Heat Resistance & Stability

With a Vicat softening point of 102°C, this High Impact HIPS resists warping under heat. Ideal for air-conditioning panels or parts near motors, maintaining structural integrity even in warm environments.

Premium Aesthetic Finish

Its high-gloss surface enhances visual appeal for consumer-facing products like appliance panels or electronics. Reduces post-processing needs while delivering a sleek, professional look.

Chimei POLYREX PH-888G

Applications

  • Indoor Air-Conditioning Panels: Heat resistance prevents warping near motors.
  • Ceiling-Mounted Extractor Fans: Impact strength handles vibrations and accidental impacts.
  • Monitor Screen Housings: High gloss eliminates secondary painting, cutting costs.
Chimei POLYREX PH-888G application

Polyrex® PH-888G Datasheet

High Gloss HIPS POLYREX® PH-888G
Product Description: High impact, High gloss
PropertiesISO Test MethodTest ConditionUnitPH-888G
Melt Flow Index1133 200℃×5KGml/10 min
Mass Density1183 23 ℃g/cm31.03 
Tensile Strength527 50 mm/min, yieldMPa35 
50 mm/min, breakMPa28 
Tensile Elongation527 50 mm/min%45 
Flexural Strength178 2 mm/minMPa48 
Flexural Modulus2 mm/minGPa2.2 
Izod Impact Strength180/1A23℃, NotchedKJ/m211 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m210 
-30℃, NotchedKJ/m25.5 
Vicat Softening Temp.306 50℃/hr;1KG102 
50℃/hr;5KG92 
Heat Distortion Temp.75/A1.8MPa, unannealed79 
1.8MPa, annealed95 
Coefficient of Linear
Thermal Expansion
11359 4~6×10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.7
Symbol1043 >PS-HI<
March 11, 2024
Notes:These are typical properties only and are not to be construed as specifications. Users
should confirm results by their own test

Polyrex® PH-888G UL Product iQ

ACRYREX® PH-888G | UL Product iQ
File Number: E56070Yellow Card™Polystyrene (PS) “POLYREX”, furnished as pellets or powder
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 3
3.0 mmPLC 3
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 0
3.0 mmPLC 0
High Voltage Arc Tracking Rate (HVTR)PLC 3
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top