Covestro Makrolon® 2407 PC Resin

Makrolon PC Polycarbonate

Makrolon® 2407 Polycarbonate PC Resin Injection molding Grade

Makrolon 2407 is a versatile, low-viscosity polycarbonate resin optimized for injection molding. With an MVR of 19 cm³/10 min (300°C/1.2 kg), UV stabilization, and easy-release properties, it processes smoothly at 280–320°C. Available in transparent, translucent, and opaque colors, it balances flow efficiency with robust performance for diverse industrial uses.

  • Character: MVR (300 °C/1.2 kg) 19 cm³/10 min; general purpose; low viscosity; UV stabilized; easy release; injection molding – melt temperature 280 – 320 °C; available in transparent, translucent and opaque colors
  • Application: Injection molding; General purpose
Please enable JavaScript in your browser to complete this form.
Click or drag files to this area to upload. You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Tensile Modulus: 2,400 MPa
  • Flexural Strength: 98 MPa
  • Notched Impact (23°C): 65 kJ/m²
  • Thermal HDT @ 1.8 MPa: 124°C
  • Vicat Softening Temp.: 143°C
  • UL 94 Rating (0.75 mm): V-2
  • CTI (Comparative Tracking Index): 250 (Solution A)
  • Volume Resistivity: 1E14 Ω·m
  • Drying Conditions: 120°C / 2–3 hrs
  • Moisture Content Max.: ≤0.02%
  • Optical Light Transmission (3mm): 88%

Features & Benefits

Superior Processing Efficiency

Covestro Makrolon 2407’s low viscosity ensures fast mold filling and shorter cycle times, reducing production costs. Ideal for complex geometries like thin-walled housings or connectors.

Exceptional Impact Resistance

With >120% strain at break and Charpy notched impact up to 65 kJ/m² (23°C), it withstands drops and impacts in automotive components, power tools, and consumer electronics.

Reliable UV & Thermal Stability

UV stabilization and heat resistance (RTI 125°C per UL 746) ensure long-term durability outdoors. Perfect for LED covers, sensors, and industrial enclosures exposed to sunlight or heat.

Application

Injection-Molded Industrial Parts

Housings, covers, and enclosures requiring clarity and toughness.

Electrical Components

Connectors, switches, and circuit breakers (UL-recognized RTI 125°C).

Consumer & Automotive

Tool handles, dash components, and outdoor fixtures (UV-stabilized).

General-Purpose Engineering

Prototypes, fasteners, and mechanical parts needing cost-effective durability.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity