Covestro Makrolon® FR6002

Makrolon PC Polycarbonate

Makrolon FR6002 PC Resin

Makrolon FR6002 by Covestro is a flame-retardant polycarbonate resin engineered for injection molding. With low viscosity (MVR 18 cm³/10 min), easy release, and UL 94 V-0 fire resistance, it ensures safety, efficiency, and reliability for high-demand industrial applications.

  • Character: flame retardant; MVR (300 °C/1.2 kg) 18 cm³/10 min; low viscosity; easy release
  • Application: Injection molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • UL 94 Rating: V-0 (0.75 mm, 1.5 mm, 3.0 mm)
  • Oxygen Index: >32%
  • Glow Wire Ignition (GVFT): 960°C
  • HDT @1.8 MPa: 124°C
  • Vicat Softening Temp: 143°C
  • CTI (Comparative Tracking Index): 250 (Solution A)
  • Volume Resistivity: 1.5 × 10¹⁵ Ω·m
  • Tensile Modulus: 2,360 MPa
  • Impact Strength (Izod Notched): 15 kJ/m²
  • Melt Temp: 280–320°C
  • Mold Temp: 80–120°C
  • Moisture Content: ≤0.02% (pre-drying essential)

Application

  • Electrical: Circuit breakers, connectors, and switch housings.
  • Automotive: Fuse boxes, sensor covers, and EV components.
  • Industrial: Machine guards, enclosures, and safety equipment.
  • Consumer Tech: Power tool casings and charger housings.

Features & Benefits

Exceptional Flame Resistance

It achieves UL 94 V-0 rating at thin walls (0.75–3.0 mm), preventing fire spread in electronics or enclosures. Ideal for safety-critical components like electrical housings.

High Mechanical Strength

It boasts 64 MPa yield stress and >50% strain at break, ensuring impact-resistant parts that withstand drops, vibrations, and heavy use in automotive/industrial settings.

Optimized Processing Efficiency

Low viscosity and easy-release properties cut cycle times during injection molding. Pre-dried at 120°C (2–3 hours), it minimizes defects for faster, cost-effective production.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity