Apec FR1897 PC Resin Heat Resistant Grade
Covestro Apec FR1897 is a flame-retardant copolycarbonate resin offering high heat resistance, UV stability, and UL 94 V-0/V-2 ratings. With low viscosity and easy mold release, itās ideal for transparent/opaque safety components like firefighter helmets.
- Character: Copolycarbonate; flame retardant, MVR (330 °C/2.16 kg) 18 cm³/10 min; low viscosity; easy release; UV stabilized (fulfills the requirements according to EN 170); V-2/1.5mm (UL 94); V-0/3.0mm (UL 94); softening temperature (VST/B 120) = 182 °C; available in transparent and opaque colors
- Application: Injection molding; Visors for firemen’s helmets
Key technical data (ISO)
- Flame Ratings: UL 94 V-0 (3.0mm), V-2 (1.5mm) | Oxygen Index: 32%
- Thermal: Vicat Softening Temp: 182°C | HDT @1.8 MPa: 157°C
- Mechanical: Tensile Strength: 72 MPa | Impact Puncture Energy: 54 J (23°C)
- Electrical: Volume Resistivity: 1E+15 Ω·m | CTI: 225 (Solution A)
- Optical: 88% Luminous Transmittance (1mm, clear grades)
- Processing: Melt Temp: 330ā340°C | Dry 3 hrs @130°C (<0.02% moisture)
Application
- Firefighter Helmet Visors: Combines transparency, UV resistance, and flame retardancy for critical PPE.
- Injection-Molded Safety Components: Electrical enclosures, automotive parts, and industrial shields requiring UL compliance.
Features & Benefits
Related ApecĀ® PC Resin Products
Covestro ApecĀ® 1897 PC Resin
Covestro ApecĀ® 1895 PC Resin
Covestro ApecĀ® 1803 PC Resin
Covestro MakrolonĀ® 1804 PC Resin
Covestro MakrolonĀ® Rx1805 RE
Covestro MakrolonĀ® 2858 RE
Covestro MakrolonĀ® 2658 RE
Covestro MakrolonĀ® 2458 RE
Covestro MakrolonĀ® 2258 RE
Covestro MakrolonĀ® Rx2530
Covestro MakrolonĀ® Rx1851
Covestro MakrolonĀ® Rx1805
Covestro MakrolonĀ® Rx1452
Covestro MakrolonĀ® 3158 PC Resin
Covestro MakrolonĀ® 2658 PC Resin
Covestro MakrolonĀ® 2558 PC Resin
Covestro MakrolonĀ® 2258 PC Resin
Covestro MakrolonĀ® 6267 X RE CQ
Advanced Manufacturing