Suke FR965 ABS Resin Flame Retardant Grade
Suke FR965 ABS resin delivers exceptional fire safety with V0 flame retardancy (1.5mm) thanks to TBBPA. Offering high flow (MFR 50 g/10min) and balanced mechanical strength, it’s the reliable choice for printers, electronics, and office equipment components.
- Manufacturer: Suke Plastics
- Character: A/TBBPA, High flame retardant
- Application: printer; Electrical &electronic; Office supplies
Key technical data (ASTM)
- Flame Retardancy: UL94 V-0 @ 1.5mm
- Melt Flow Rate (MFR): 50 g/10 min (220°C / 10.0 kg)
- Density: 1.19 g/cm³
- Tensile Strength: 40 MPa
- Flexural Strength: 68 MPa
- Flexural Modulus: 2100 MPa
- Impact Strength (Izod Notched): 18 kJ/m² (3.2mm, 23°C)
- Heat Deflection Temp (HDT): 77 °C (@ 0.45 MPa, 6.4mm)
- Processing Drying: 80°C for 3 hours recommended
- Processing Melt Temperature: ~200°C
- Processing Max Processing Temp: 220°C
- Processing Mold Temperature: ~70°C
Application
- Printer Components: Housings, internal frames, paper trays, covers.
- Electrical & Electronic Parts: Connectors, sockets, enclosures, internal supports, terminal blocks.
- Office Supplies: Copier housings, computer accessory casings, equipment covers, robust organizers.

Features & Benefits

Related Suke ABS resin Products