Suke Plastics FR965C ABS Resin

Suke Plastics Modified Plastic

Suke FR965C ABS Resin Flame Retardant Grade

Suke FR965C is a high-performance ABS resin engineered with TBBPA-based flame retardancy, achieving UL94 V-0 compliance at just 2.0mm thickness. Ideal for electronics and office equipment, it combines rigorous safety standards with reliable processability for high-volume manufacturing.

  • Manufacturer: Suke Plastics
  • Character: A/TBBPA, flame retardant
  • Application: Electrical &electronic; Office supplies
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ASTM)

  • Flame Rating: UL94, V-0 (2.0mm)
  • Melt Flow Rate: 50 g/10min
  • Tensile Strength: 40 MPa
  • Impact Strength: 21 kJ/m²
  • Heat Deflection Temp: 77°C (0.45MPa)
  • Density: 1.19 g/cm³
  • Mold Shrinkage: INTERNAL, 0.4–0.7%
  • Processing Injection Pressure: 60–100 MPa
  • Processing Melt Temp: 200°C (Max 220°C)
  • Processing Mold Temp: 70°C

Application

  • Electronics & Electrical: Circuit breakers, connectors, power tool housings.
  • Office Supplies: Printer components, scanner frames, ergonomic device casings.
Suke FR965C ABS plastic application
Suke FR965C ABS plastic

Features & Benefits

Guaranteed Fire Safety

It meets UL94 V-0 flammability standards (2.0mm), significantly reducing fire risks in electronics. Essential for compliance-sensitive applications like power strips and server housings.

Optimized Production Efficiency

High melt flow rate (50 g/10min @220°C) ensures fast injection molding with minimal energy. Pre-dries in 3 hours at 80°C, cutting downtime for urgent orders.

Balanced Mechanical Strength

It retains 40 MPa tensile strength and 21 kJ/m² impact resistance despite flame-retardant additives. Prevents brittle failures in thin-walled components like laptop casings.

Suke FR965C ABS resin
Suke FR965C ABS resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity