Lexan 101 general Purpose Grade
Lexan PC Resin 101 is a versatile 7 MFR polycarbonate, ideal for both extrusion and injection molding. It offers an outstanding balance of high impact strength, clarity, and thermal resistance, perfect for demanding industrial applications.
- Character: a 7 MFR polycarbonate, MVR of 6. UL94 HB rated.
Key technical data
- Tensile Strength at Yield: 62 MPa
- Flexural Modulus: 2340 MPa
- Notched Izod Impact (23°C): 907 J/m
- Heat Deflection Temp (HDT) @ 1.82 MPa: 132°C
- Vicat Softening Temperature: 154°C
- Relative Temperature Index (Electrical/Mech): 130°C
- Light Transmission (2.54mm): 88%
- Haze (2.54mm): 1%
- Specific Gravity: 1.20
- Mold Shrinkage: 0.5 – 0.7%
- Flame Rating UL94 Rating: HB
- Melt Flow Rate (300°C/1.2kg): 7 g/10 min
- Melt Temperature: 310 – 330°C
Application
- Automotive Components
- Consumer Electronics Housings
- Electrical Enclosures and Connectors
- Industrial Parts and Equipment
- And other specialized applications requiring a high-flow, tough polycarbonate base.
Features & Benefits

Related Lexan™ Polycarbonate Products
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
LEXAN™ PC Resin AVP TLL12CU
LEXAN™ PC Resin AVP KLL10FR
LEXAN™ PC Resin AT2030R
LEXAN™ PC Resin AT1230R
LEXAN™ PC Resin 244RF
LEXAN™ PC Resin AD143
LEXAN™ PC Resin 263R
Advanced Manufacturing