Sabic LEXAN™ PC Resin AD143

sabic pc resin 25kg package

SABIC Lexan AD143 Flame Retardant Grade

LEXAN™ LEXAN™ Resin AD143 is a medium-viscosity, injection molding-grade PC material offering exceptional optical clarity, high light transmission, and low dust attraction. It is the ideal engineering thermoplastic for applications demanding both visual excellence and reliable performance, available in both transparent and opaque colors.AD143

Associated Documents

TDS Asia

Typical property data

Physical Properties
  • Specific Gravity: 1.2 (ASTM D792)
  • Density: 1.2 g/cm³ (ISO 1183)
  • Mold Shrinkage (flow): 0.5 – 0.7% (SABIC method)
  • Melt Flow Rate (300°C/1.2 kgf): 13 g/10 min (ASTM D1238)
  • Water Absorption (23°C, saturated): 0.35% (ISO 62-1)
  • Moisture Absorption (23°C, 50% RH): 0.15% (ISO 62)
Mechanical Properties
  • Tensile Stress (yield): 63 MPa (ISO 527)
  • Tensile Stress (break): 70 MPa (ISO 527)
  • Tensile Strain (yield): 6% (ISO 527)
  • Tensile Strain (break): 120% (ISO 527)
  • Tensile Modulus: 2350 MPa (ISO 527)
  • Flexural Stress (yield): 90 MPa (ISO 178)
  • Flexural Modulus: 2300 MPa (ISO 178)
  • Ball Indentation Hardness: 95 MPa (ISO 2039-1)
Impact Properties
  • Izod Impact (notched, 23°C): 70 kJ/m² (ISO 180/1A)
  • Izod Impact (unnotched, 23°C): No Break (ISO 180/1U)
  • Charpy Impact (V-notch, -30°C): 14 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Vicat Softening Temperature (Rate B/50): 140 °C (ISO 306)
  • Heat Deflection Temperature (HDT, 1.8 MPa): 123 °C (ISO 75/Ae)
  • Thermal Conductivity: 0.2 W/m-°C (ISO 8302)
  • Coefficient of Thermal Expansion (CTE, 23°C to 80°C, flow): 7.E-05 1/°C (ISO 11359-2)
Optical Properties
  • Light Transmission (2.54 mm): 89% (ASTM D1003)
  • Haze (2.54 mm): <0.8% (ASTM D1003)
  • Refractive Index: 1.586 (ISO 489)
Electrical Properties

Surface Resistivity: 5.E+13 Ω (ASTM D257)

Flame Characteristics

Glow Wire Flammability Index: 850°C, passes at 1.6 mm (IEC 60695-2-12)

Injection Molding
  • Drying Temperature: 120 °C
  • Drying Time: 2 – 4 hours
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 280 – 310 °C
  • Mold Temperature: 80 – 110 °C

Features & Benefits

Superior Optical Clarity

With 89% light transmission and extremely low haze (<0.8%), LEXAN AD143 produces crystal-clear parts. This ensures vibrant, distortion-free visibility for lenses, covers, and displays, enhancing product aesthetics and user experience.

High Impact & Mechanical Strength

This resin delivers outstanding toughness, even at low temperatures. Its high notched Izod impact strength reduces the risk of cracking or failure from drops or impacts, leading to more durable and longer-lasting components.

Excellent Thermal Stability

Featuring a high Heat Deflection Temperature (HDT up to 130°C), LEXAN AD143 maintains structural integrity in elevated temperature environments. This allows for reliable performance in applications exposed to heat, such as under-hood automotive parts or sterilizable medical devices.