SABIC PC Lexan 123R General Purpose Grade
SABIC Lexan 123R is a versatile, high-performance polycarbonate resin. This 18 MFR material is UV stabilized, contains a mold release, and carries key UL ratings for electrical and flame safety.
- Character: 18 MFR polycarbonate, MVR of 21. UV Stabilized. Mold release. UL746C f1 rated. UL94 HB rated
Key technical data
- Tensile Strength at Yield: 62 MPa
- Flexural Modulus: 2340 MPa
- Notched Izod Impact (23°C): 694 J/m
- Rockwell Hardness (M Scale): 70
- Heat Deflection Temp (1.82 MPa): 132 °C
- Vicat Softening Temperature: 154 °C
- Relative Temperature Index (Elec/Mech): 130 °C
- Volume Resistivity: >1E+17 Ω·cm
- Dielectric Strength: 14.9 kV/mm
- Comparative Tracking Index (CTI): PLC 2
- Melt Temperature: 280 – 305 °C
- Mold Temperature: 70 – 95 °C
- Light Transmission (2.54mm): 88%
- UL94 Flame Class Rating: HB @ 0.76 mm
Application
- Electrical housings and enclosures
- Automotive interior and exterior components
- Protective covers and shields
- Consumer appliance parts
- Various industrial components
Features & Benefits

Related Lexan™ Polycarbonate Products
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
LEXAN™ PC Resin AVP TLL12CU
LEXAN™ PC Resin AVP KLL10FR
LEXAN™ PC Resin AT2030R
LEXAN™ PC Resin AT1230R
LEXAN™ PC Resin 244RF
LEXAN™ PC Resin AD143
LEXAN™ PC Resin 263R
Advanced Manufacturing