LEXAN™ PC Resin 143R

LEXAN™ PC Resin Sabic Tianjin

SABIC PC Lexan 143R General Purpose Grade

SABIC Lexan 143R is a versatile, UV-stabilized polycarbonate resin. It offers an excellent balance of high impact strength, clarity, and ease of processing with a built-in mold release, ideal for demanding applications across various industries.

  • Character: 11 MFR polycarbonate, MVR of 12. UV Stabilized. Mold release. UL94 HB rated. UL746C f1 rated.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Stress at Yield: 62 MPa
  • Flexural Modulus: 2340 MPa
  • Notched Izod Impact (23°C): 801 J/m
  • Heat Deflection Temp (1.82 MPa): 132°C
  • Vicat Softening Temperature: 154°C
  • Relative Temperature Index (Elec/Mech): 130°C
  • Light Transmission (2.54mm): 88%
  • Haze (2.54mm): 1%
  • Specific Gravity: 1.20
  • Mold Shrinkage: 0.5 – 0.7%
  • UL94 Flame Rating: HB (0.76 mm)
  • Volume Resistivity: >1E+17 Ω·cm
  • Melt Temperature: 295 – 315°C
  • Mold Temperature: 70 – 95°C
  • Drying: 3-4 hours at 120°C

Application

  • Automotive interior components (e.g., lens covers, glove box doors)
  • Transparent protective shields and machine guards
  • Housings for consumer electronics and power tools
  • Lighting components and diffusers
  • Medical device housings (non-implant)
  • Various industrial and consumer durable goods

Features & Benefits

Superior Impact Resistance & Clarity

With exceptional notched Izod impact strength, components resist cracking and breaking during use or assembly. Its high light transmission makes it perfect for durable, see-through covers and lenses.

Built-In Mold Release Agent

This feature significantly improves production efficiency by allowing for easier part ejection from the mold. It reduces cycle times and potential mold fouling, lowering your overall part cost.

Excellent UV & Thermal Stability

The resin is UV stabilized, ensuring long-term color and property retention outdoors. It maintains performance at high temperatures, suitable for applications exposed to heat and sunlight.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top