SABIC LEXAN 101R resin is a versatile, high-performance polycarbonate. With a UL HB rating and 7.0 MFR, it offers excellent flow for thick-walled parts without sink marks, simplifying your production.

  • Character: UL HB rating and 7.0 MFR
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 62 MPa
  • Flexural Modulus: 2340 MPa
  • Notched Izod Impact (23°C): 907 J/m
  • Heat Deflection Temp (1.82 MPa): 132°C
  • Vicat Softening Temperature: 154°C
  • Relative Temperature Index (Elec/Mech): 130°C
  • Light Transmission (2.54mm): 88%
  • Specific Gravity: 1.20
  • UL 94 Flame Rating: HB (0.71 mm)
  • Volume Resistivity: >1.E+17 Ω·cm
  • Melt Temperature: 310 – 330°C
  • Mold Temperature: 80 – 115°C
  • Drying Time: 3-4 hours at 120°C

Application

  • Thick-walled electrical enclosures and housings.
  • Industrial components requiring high strength and dimensional stability.
  • Consumer and automotive parts where durability is critical.
  • Any application benefiting from easy demolding and reduced cycle times.

Features & Benefits

Excellent Processability with Internal Release

This grade contains an internal mold release agent, which facilitates faster cycle times and easier part ejection, boosting your production efficiency and reducing downtime for mold maintenance.

Superior Impact Resistance and Toughness

It delivers outstanding notched Izod impact strength, ensuring your components can withstand sudden impacts, drops, and rough handling, resulting in durable and reliable end-products.

High Clarity for Functional Applications

The material provides high light transmission and low haze, making it ideal for applications requiring visual inspection or light transmission, without the need for more expensive optical grades.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top