SABIC PC Lexan 104 General Purpose Grade
LEXAN 104 is a versatile 7 MFR polycarbonate resin, UL94 HB rated. It is engineered for high performance in both extrusion and injection molding, and is designed for food contact applications, meeting global compliance needs.
- Character: 7 MFR, UL94 HB rated, for food contact applications
Key technical data
- Tensile Strength at Break: 68 MPa
- Flexural Modulus: 2340 MPa
- Notched Izod Impact (23°C): 907 J/m
- Rockwell Hardness (M Scale): 70
- Heat Deflection Temp (1.82 MPa): 132 °C
- Vicat Softening Temperature: 154 °C
- Relative Temperature Index (Elec/Mech): 130 °C
- Melt Flow Rate (300°C/1.2kg): 7 g/10 min
- Mold Shrinkage: 0.5 – 0.7 %
- Light Transmission (2.54mm): 88%
- Specific Gravity: 1.20
- UL94 Rating: HB (1.47 mm)
- Volume Resistivity: >1.E+17 Ω·cm
- Dielectric Strength: 14.9 kV/mm
Application
- Food storage containers and packaging
- Kitchenware and utensils
- Medical device housings and components
- Protective glazing and sight glasses
- Consumer goods components
- Various extruded profiles and injection molded parts
Features & Benefits

Related Lexan™ Polycarbonate Products
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
LEXAN™ PC Resin AVP TLL12CU
LEXAN™ PC Resin AVP KLL10FR
LEXAN™ PC Resin AT2030R
LEXAN™ PC Resin AT1230R
LEXAN™ PC Resin 244RF
LEXAN™ PC Resin AD143
LEXAN™ PC Resin 263R
Advanced Manufacturing