LEXAN™ PC Resin 104R

LEXAN™ PC Resin Sabic Tianjin

SABIC PC Lexan 104R General Purpose Grade

LEXAN 104R is a versatile 7 MFR polycarbonate resin. It features a mold release agent, a UL94 HB rating, and is suitable for both injection molding and extrusion, offering excellent food contact compliance.

  • Character: 7 MFR, UL94 HB rating
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Tensile Strength at Yield: 62 MPa
  • Flexural Modulus: 2340 MPa
  • Notched Izod Impact (23°C): 907 J/m
  • Heat Deflection Temp (1.82 MPa): 132°C
  • Vicat Softening Temperature: 154°C
  • Specific Gravity: 1.20
  • Light Transmission (2.54mm): 88%
  • Haze (2.54mm): 1%
  • UL Relative Temperature Index (Elec/Mech): 130°C
  • Flammability Rating: UL 94 HB
  • Melt Temperature: 310 – 330°C
  • Mold Temperature: 80 – 115°C
  • Recommended Moisture Content: < 0.02%

Application

  • Injection Molding Applications
  • Extrusion Applications

Features & Benefits

Excellent Impact Resistance & Toughness

With its high notched Izod impact strength, this LEXAN™ 104R resin creates durable products that withstand accidental drops and impacts, reducing breakage and returns.

High Clarity for Functional Applications

The material offers 88% light transmission with very low haze, ideal for applications like food containers or machine sight glasses where visual inspection is important.

Reliable Thermal Performance

Maintaining mechanical properties at elevated temperatures, it is perfect for components in appliances and electrical housings that encounter heat during use or processing.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top