LEXAN™ PC Resin 123M

LEXAN™ PC Resin Sabic Tianjin

SABIC PC Lexan 123M General Purpose Grade

LEXAN 123M is a versatile 18 MFR polycarbonate resin. It features UV stabilization, improved internal mold release for faster cycles, and a UL94 HB flammability rating for reliable performance.

  • Character: 18 MFR, UV Stabilized, UL94 HB rated.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength at Yield: 63 MPa
  • Flexural Modulus: 2350 MPa
  • Notched Izod Impact (23°C): 820 J/m
  • Heat Deflection Temp (1.82 MPa): 132 °C
  • Vicat Softening Temperature: 143 °C
  • Melt Flow Rate (300°C/1.2kg): 17.5 g/10 min
  • Mold Shrinkage: 0.5 – 0.8 %
  • UL94 Flammability Rating: HB
  • Light Transmission (2.54mm): 88%

Application

  • Electrical enclosures and components
  • Automotive interior and exterior trim
  • Consumer electronics housings
  • Lighting fixtures and covers
  • Industrial machine guards
  • Transparent or tinted safety panels
  • Small appliance parts
  • Business equipment casings

Features & Benefits

Fast, Efficient Moldability

With an 18 MFR, SABIC LEXAN 123M enables faster cycle times and easier flow into intricate molds—ideal for high-volume production with tight tolerances.

Built-In UV Stability

LEXAN™ 123M resin resists yellowing and degradation from sunlight, making it ideal for outdoor or light-exposed parts like electrical housings or automotive trim.

Improved Internal Mold Release

Its self-releasing formulation reduces the need for external mold-release agents, minimizing part defects and reducing downtime in manufacturing.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity