SABIC PC Lexan 131 General Purpose Grade
LEXAN 131 is a versatile 3.5 MFR polycarbonate resin, UL94 HB rated. It is engineered for high performance in blow molding, extrusion, and injection molding processes, offering an excellent balance of clarity, impact strength, and thermal resistance.
- Character: 3.5 MFR, UL94 HB rated
Key technical data
- Tensile Strength at Break: 65 MPa
- Flexural Modulus: 2340 MPa
- Notched Izod Impact (23°C): 907 J/m
- Rockwell Hardness (M Scale): 70
- Heat Deflection Temperature (HDT) @ 1.82 MPa: 132°C
- Vicat Softening Temperature: 154°C
- Relative Temperature Index (Electrical): 125°C
- Melt Flow Rate (300°C/1.2kg): 3.5 g/10 min
- Mold Shrinkage: 0.5 – 0.7%
- Specific Gravity: 1.20
- Water Absorption (24hr): 0.15%
- Light Transmission (2.54mm): 88%
- Haze (2.54mm): 1%
- Volume Resistivity: >1E+17 Ω·cm
- Flammability Rating: UL 94 HB
Application
- Durable consumer product housings
- Automotive interior parts
- Electrical components and covers
- Clear protective shields and lenses
- Various industrial parts requiring toughness and clarity
Features & Benefits

Related Lexan™ Polycarbonate Products
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
LEXAN™ PC Resin AVP TLL12CU
LEXAN™ PC Resin AVP KLL10FR
LEXAN™ PC Resin AT2030R
LEXAN™ PC Resin AT1230R
LEXAN™ PC Resin 244RF
LEXAN™ PC Resin AD143
LEXAN™ PC Resin 263R
Advanced Manufacturing