LEXAN™ PC Resin 141

LEXAN™ PC Resin Sabic Tianjin

SABIC PC Lexan 141 General Purpose Grade

LEXAN 141 is a versatile 11 MFR polycarbonate resin, UL94 HB rated. It delivers an exceptional balance of high impact strength, clarity, and thermal resistance.

  • Character: 11 MFR, UL94 HB rated
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Tensile Strength at Yield: 62 MPa
  • Flexural Modulus: 2340 MPa
  • Notched Izod Impact (23°C): 801 J/m
  • Rockwell Hardness (M Scale): 70
  • Heat Deflection Temperature (HDT) @ 0.45 MPa: 137°C
  • Vicat Softening Temperature: 154°C
  • Relative Temperature Index (RTI): 130°C
  • Light Transmission (2.54mm): 88%
  • Haze (2.54mm): 1%
  • Specific Gravity: 1.20
  • Mold Shrinkage: 0.5 – 0.7%
  • Volume Resistivity: >1.5E+17 Ω·cm
  • Dielectric Strength: 14.9 kV/mm
  • Melt Temperature: 295 – 315°C
  • Mold Temperature: 70 – 95°C
  • Drying: 3-4 hours at 120°C

Application

  • Consumer Electronics Housings and Components
  • Automotive Interior Trim and Components
  • Transparent Covers, Shields, and Lenses
  • Lighting Components and Diffusers
  • Various Durable Goods and Appliances

Features & Benefits

Superior Impact Resistance & Toughness

With an exceptional notched Izod impact of 801 J/m, LEXAN™ 141 withstands sudden impacts and rough handling, reducing part breakage and ensuring product longevity in demanding environments.

Excellent Clarity and Light Transmission

This resin offers 88% light transmission with low haze, providing crystal-clear visibility. It’s ideal for lenses, covers, and displays where optical quality and an attractive appearance are critical.

High Heat Resistance & Stability

Featuring a Heat Deflection Temperature of 137°C, SABIC LEXAN 141 maintains its structural integrity under elevated temperatures, ensuring reliable performance in applications exposed to heat or hot environments.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top