LEXAN™ PC Resin 143

LEXAN™ PC Resin Sabic Tianjin

SABIC PC Lexan 143 General Purpose Grade

LEXAN 143 is a UV-stabilized, non-halogenated polycarbonate resin with a 10.5 MFR and a UL HB flame rating. This versatile, high-performance material offers an exceptional balance of impact strength, clarity, and thermal resistance for demanding engineering applications.

  • Character: 10.5 MFR. UV-stabilized.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength (Yield): 62 MPa
  • Flexural Modulus: 2340 MPa
  • Izod Impact, Notched: 801 J/m
  • Rockwell Hardness (M Scale): 70
  • Heat Deflection Temp (HDT @ 1.82 MPa): 132°C
  • Vicat Softening Point: 154°C
  • Relative Temperature Index (RTI): 130°C
  • Melt Flow Rate (300°C/1.2kg): 10.5 g/10 min
  • Specific Gravity: 1.20
  • Mold Shrinkage: 0.5 – 0.7%
  • Moisture Content (Max for Processing): 0.02%
  • Light Transmission (2.54mm): 88%
  • Haze: 1%
  • UL94 Flame Rating: HB (0.76 mm)
  • Dielectric Strength: 14.9 kV/mm
  • Volume Resistivity: >1E+17 Ω·cm

Application

  • Automotive
  • Electrical & Electronics
  • Consumer & IT
  • Industrial

Features & Benefits

Exceptional Impact Resistance

With an unmatched notched Izod impact of 801 J/m, LEXAN™ 143 withstands severe shocks and drops that would crack or shatter ordinary plastics.

High Heat & Dimensional Stability

Featuring a Heat Deflection Temperature (HDT) of 132°C at 1.82 MPa, this resin maintains its shape and strength under high thermal stress.

Crystal Clarity & UV Stability

Offering 88% light transmission with low haze, LEXAN™ 143 provides excellent optical clarity. Its built-in UV stabilizer protects against yellowing and degradation.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity