SABIC PC Lexan 144R General Purpose Grade
LEXAN 144R is a versatile, high-flow polycarbonate resin designed for ease of processing. It features built-in mold release, a UL94 HB flame rating, and is compliant for food contact in most regions.
- Character: 11 MFR, MVR of 12. Mold release. UL94 HB rated.
Key technical data
- Tensile Strength at Yield: 62 MPa
- Flexural Modulus: 2340 MPa
- Izod Impact (Notched): 801 J/m
- Rockwell Hardness (M Scale): 70
- Heat Deflection Temp (HDT) @ 1.82 MPa: 132°C
- Vicat Softening Temperature: 154°C
- Relative Temperature Index: 130°C
- Specific Gravity: 1.20
- Mold Shrinkage: 0.5 – 0.7%
- Light Transmission (2.54mm): 88%
- Haze (2.54mm): 1%
- Flame Rating: UL 94 HB
- Melt Temperature: 295 – 315°C
- Mold Temperature: 70 – 95°C
- Drying: 3-4 hours at 120°C
Application
- Consumer & Household Goods
- Electrical & Enclosures
- Industrial & General Components
- Healthcare & Lifestyle
Features & Benefits

Related Lexan™ Polycarbonate Products
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
LEXAN™ PC Resin AVP TLL12CU
LEXAN™ PC Resin AVP KLL10FR
LEXAN™ PC Resin AT2030R
LEXAN™ PC Resin AT1230R
LEXAN™ PC Resin 244RF
LEXAN™ PC Resin AD143
LEXAN™ PC Resin 263R
Advanced Manufacturing