SABIC PC Lexan 153R General Purpose Grade
LEXAN 153R is a versatile, UV-stabilized polycarbonate resin engineered for high-performance blow molding and extrusion. With built-in mold release and a UL94 HB flame rating, it offers excellent durability, clarity, and processing ease for demanding industrial applications.
- Character: 2.5 MFR Branched polycarbonate. UV Stabilized. Mold release. UL94 HB rated.
Key technical data
- Tensile Strength (Yield): 62 MPa
- Flexural Modulus: 2340 MPa
- Izod Impact (Notched): 747 J/m
- Rockwell Hardness (M Scale): 70
- Heat Deflection Temp (HDT @ 1.82 MPa): 132 °C
- Vicat Softening Temperature: 157 °C
- Melt Flow Rate (300°C/1.2kg): 2.5 g/10 min
- Specific Gravity: 1.2
- Water Absorption (24hr): 0.15%
- Mold Shrinkage: 0.5 – 0.7%
- Light Transmission (2.54mm): 88%
- Haze: 1%
- Flame Rating: UL94 HB
Application
- Blow Molding
- Extrusion
Features & Benefits

Related Lexan™ Polycarbonate Products
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
LEXAN™ PC Resin AVP TLL12CU
LEXAN™ PC Resin AVP KLL10FR
LEXAN™ PC Resin AT2030R
LEXAN™ PC Resin AT1230R
LEXAN™ PC Resin 244RF
LEXAN™ PC Resin AD143
LEXAN™ PC Resin 263R
Advanced Manufacturing