SABIC PC Lexan 161R General Purpose Grade
LEXAN 161R is a versatile, medium-viscosity polycarbonate resin engineered for easy processing. Formulated with an integrated release agent, it ensures excellent mold flow and is available in transparent, translucent, and opaque color options for maximum design flexibility.
- Character: medium viscosity multi purpose grade
Key technical data
- Tensile Strength (Yield): 63 MPa
- Tensile Modulus: 2350 MPa
- Izod Impact, Notched (23°C): 70 kJ/m²
- Flexural Modulus: 2300 MPa
- Heat Deflection Temperature (HDT @ 1.8 MPa): 127°C
- Vicat Softening Temperature (Rate B/50): 143°C
- Relative Temperature Index (Electrical): 130°C
- Volume Resistivity: >1.E+15 Ω·cm
- Comparative Tracking Index (CTI): 225 V
- Dielectric Strength (0.8mm): 35 kV/mm
- UL 94 Flame Rating: HB (1.1 mm & 3.0 mm)
- Density: 1.20 g/cm³
- Mold Shrinkage: 0.5 – 0.7 %
- Light Transmission (2.54mm): 88 – 90 %
- Water Absorption (Saturated): 0.35 %
- Melt Temperature: 280 – 310 °C
- Mold Temperature: 80 – 110 °C
- Drying: 2-4 hours at 120°C
Download
Application
- Automotive interior and exterior components
- Electrical housings and enclosures
- Consumer electronics casings
- Transparent safety shields and covers
- Lighting components (translucent/transparent versions)
- Industrial equipment housings
- Medical device housings (non-implantable)
- Office equipment and printer components
Features & Benefits

Related Lexan™ Polycarbonate Products
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
LEXAN™ PC Resin AVP TLL12CU
LEXAN™ PC Resin AVP KLL10FR
LEXAN™ PC Resin AT2030R
LEXAN™ PC Resin AT1230R
LEXAN™ PC Resin 244RF
LEXAN™ PC Resin AD143
LEXAN™ PC Resin 263R
Advanced Manufacturing