SABIC Lexan EX8681T coextrusion PC
LEXAN™ Resin EX8681T is a premium, coextrudable polycarbonate resin engineered for exceptional long-term performance in demanding outdoor environments. Its high UV stabilization ensures superior weathering resistance and color retention for LEXAN™ sheet, combined with excellent processability.
- Character: coextrusion, highly UV stabilized
Typical property data
Mechanical Properties
- Tensile Strength (Yield): 63 MPa
- Tensile Modulus: 2350 MPa
- Flexural Strength (Yield): 90 MPa
- Flexural Modulus: 2300 MPa
- Elongation at Break: 120%
Physical Properties
- Density: 1.2 g/cm³
- Melt Volume Rate (300°C/1.2 kg): 10 cm³/10 min
Thermal Properties
- Vicat Softening Temperature (B/120): 135°C
Processing Guideline
- Drying: 105°C for 2-3 hours
- Melt Temperature Range: 220 – 250°C
- Die Temperature Range: 245 – 290°C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin EX8681T
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
LEXAN™ PC Resin AVP TLL12CU
LEXAN™ PC Resin AVP KLL10FR
LEXAN™ PC Resin AT2030R
LEXAN™ PC Resin AT1230R
LEXAN™ PC Resin 244RF
LEXAN™ PC Resin AD143
Advanced Manufacturing