LEXAN™ PC Resin EX9332T

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan EX9332T high-viscosity

LEXAN™ Resin EX9332T is a high-viscosity, branched polycarbonate engineered for demanding extrusion applications. It combines inherent flame retardancy, UV stabilization, and excellent impact resistance, making it an ideal, durable material for critical sectors like railway systems and architectural construction, where long-term performance and safety are paramount.

  • Character: high viscosity, branched, extrusion, flame retadant, mold release, UV stabilized
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength (Yield): 65 MPa
  • Flexural Modulus: 2350 MPa
  • Ball Indentation Hardness: 95 MPa

Impact Properties

  • Notched Izod Impact (23°C): 11 kJ/m²
  • Notched Charpy Impact (23°C): 11 kJ/m²
  • Unnotched Impact: No Break (NB) at both 23°C and -30°C

Thermal Properties

  • Heat Deflection Temperature (HDT/A @1.8 MPa): 135°C
  • Vicat Softening Temperature (Rate B/50): 155°C
  • Continuous Use Temperature (Relative Temp Index): 80°C

Physical Properties

  • Density: 1.25 g/cm³
  • Light Transmission (2.54mm): 88%
  • Water Absorption (Saturated): 0.32%
  • Mold Shrinkage: 0.4 – 0.6%

Flame Performance

  • UL 94 Rating: V-0 at 1.5 mm thickness
  • Oxygen Index (LOI): 37%
  • Glow-Wire Ignitability Temperature (GWIT): 850°C

Processing Guidelines

  • Drying: 120°C for 2-4 hours
  • Melt Temperature: 260 – 300°C
  • Barrel Temperature Range: 260 – 300°C

Features & Benefits

Inherent Flame Retardancy & Safety

LEXAN EX9332T achieves a UL 94 V-0 rating, providing critical fire safety for public transport and buildings, reducing risk and helping meet stringent regulatory requirements.

Exceptional Toughness & Durability

Its superior impact resistance, even at -30°C, ensures components resist cracking and vandalism, delivering long service life and reliability in demanding outdoor and structural applications.

Weatherability & Dimensional Stability

UV-stabilized formulation protects against yellowing and degradation from sunlight, while low moisture absorption and a consistent CTE ensure parts maintain their shape and fit over time.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top