LEXAN™ PC Resin GLX143

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan GLX143 Medium viscosity grade

LEXAN™ Resin GLX143 is a medium-viscosity polycarbonate designed for applications demanding high optical clarity and strength. Ideal for automotive glazing, it offers excellent transparency, impact resistance, and processing flexibility in both transparent and translucent colors.

  • Character: MVR of 12. Medium viscosity grade
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength: 60 MPa
  • Flexural Strength: 90 MPa
  • Flexural Modulus: 2,400 MPa

Impact Properties

  • Notched Izod Impact (23°C): 65 kJ/m²
  • Unnotched Izod Impact (23°C): No Break

Thermal Properties

  • Heat Deflection Temperature (1.8 MPa): 130°C
  • Vicat Softening Temperature: 145°C

Physical Attributes

  • MVR (300°C/1.2 kg): 12 cm³/10 min
  • Density: 1.2 g/cm³

Flame Performance

  • UL94 Rating: V2 at 1.5 mm

Processing Guidelines

  • Recommended Melt Temperature: 280–310°C
  • Mold Temperature: 80–100°C
  • Drying Conditions: 120°C for 4 hours

Features & Benefits

High Optical Clarity

LEXAN GLX143 delivers exceptional transparency, making it ideal for automotive windows and panels requiring clear visibility and aesthetic appeal.

Outstanding Impact Strength

Engineered to withstand high mechanical stress, this resin offers superior impact resistance—critical for safety in vehicle glazing and exterior panels.

Versatile Processing Performance

With a balanced flow rate and excellent thermal stability, LEXAN Resin GLX143 supports efficient molding, reducing cycle times and manufacturing costs.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top