SABIC Lexan HF1130R UV-stabilized
LEXAN™ Resin HF1130R is a high-flow, UV-stabilized polycarbonate designed for precision molding. It has excellent dimensional stability, flame resistance (UL94 V2), and easy mold release. Ideal for outdoor and electrical applications.
- Character: 25 MFR, MVR of 26. UV stabilized
Typical property data
Mechanical Properties
- Tensile Strength @ Yield: 60 MPa
- Flexural Strength: 90 MPa
- Flexural Modulus: 2,300 MPa
- Tensile Modulus: 2,300 MPa
Impact Properties
- Izod Notched Impact (23°C): 65 J/m
- Izod Unnotched Impact (23°C): No Break
- Charpy Unnotched Impact: No Break
Thermal Properties
- Heat Deflection Temp (1.8 MPa): 125°C
- Vicat Softening Point: 145°C
- Thermal Expansion Coefficient: 6.5 x 10⁻⁵ /°C
Physical Properties
- Mold Shrinkage: 0.5 – 0.7%
- Specific Gravity: 1.2
- MVR (300°C/1.2kg): 26 cm³/10 min (25 MFR grade)
- Color: Natural
- UV Stabilized: Yes
- Mold Release: Yes
Flame Performance
- UL94 Flame Rating: V2 @ 1.5 mm and 3.0 mm
- Glow Wire Ignition Temperature (GWIT): 750°C
- Glow Wire Flammability Index (GWFI): 850°C
Processing Guidelines
- Recommended Mold Temperature: 80–120°C
- Processing Temperature: 280–310°C
- Drying Temperature: 120°C for 3–4 hours
- Moisture Content Before Processing: <0.02%
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin HF1130R
LEXAN™ PC Resin HF1130
LEXAN™ PC Resin HF1110R
LEXAN™ PC Resin HF1110
LEXAN™ PC Resin GLX143
LEXAN™ PC Resin EX9332T
LEXAN™ PC Resin EX8681T
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
LEXAN™ PC Resin EX1632T
LEXAN™ PC Resin EX1332T
LEXAN™ PC Resin EM1210
Advanced Manufacturing