LEXAN™ PC Resin HF1140R

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan HF1140R High Flowstabilized

LEXAN™ Resin HF1140R is a high-flow polycarbonate designed for efficient molding, flame resistance (UL94 V2), and food contact compliance. Ideal for applications requiring clarity, strength, and safety in regulated environments such as food processing and consumer goods.

  • Character: 25 MFR, MVR of 26. Mold release. UL94 V2 rated.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength at Yield: 60 MPa
  • Flexural Strength: 90 MPa
  • Flexural Modulus: 2,300 MPa
  • Tensile Modulus: 2,300 MPa

Impact Properties

  • Notched Izod Impact (23°C): 60 J/m

Thermal Properties

  • Heat Deflection Temperature (0.45 MPa): 138°C
  • Heat Deflection Temperature (1.8 MPa): 125°C
  • Vicat Softening Temperature (B/120): 145°C

Physical Properties

  • Specific Gravity: 1.20
  • Mold Shrinkage: 0.5 – 0.7%
  • MVR (300°C/1.2kg): 26 cm³/10 min

Flame Performance

  • UL94 Flame Rating: V-2 @ 1.5 mm and 3.0 mm

Processing Guidelines

  • Melt Temperature: 280–310°C
  • Mold Temperature: 80–110°C
  • Drying Conditions: 120°C for 2–4 hours

Features & Benefits

High Flow for Complex Molding

With a melt volume rate of 26, LEXAN HF1140R ensures fast, consistent flow—ideal for intricate or multi-cavity molds.

Food Contact Compliance

Certified for food contact in most jurisdictions, it’s a safe and reliable choice for applications in food service equipment and packaging.

Flame Resistance Built In

UL94 V-2 rating provides essential flame retardancy, helping manufacturers meet safety standards in regulated industries.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity