SABIC Lexan HF1840R High Flow
LEXAN™ Resin HF1840R is a transparent, low-viscosity polycarbonate resin engineered for high-flow injection molding. With excellent mold release and food contact compliance in most regions, it’s ideal for precision parts in regulated industries like food packaging and consumer goods.
- Character: extreme low viscosity, injection molding, mold release, transparent.
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 60 MPa
- Flexural Modulus: 2,200 MPa
- Elongation at Break: 110%
Impact Properties
- Notched Izod Impact (23°C): 65 kJ/m²
- Unnotched Izod Impact (23°C): No Break
Thermal Properties
- Vicat Softening Temperature: 148°C
Physical Properties
- Transparency: High clarity
- Density: 1.2 g/cm³
- Mold Release: Enhanced for complex geometries
Flame Performance
- UL94 Rating: V2 at 1.5 mm
Processing Guidelines
- MVR (300°C/1.2kg): 36 cm³/10min
- Processing Method: Injection Molding
- Recommended Mold Temperature: 80–120°C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin HF1840R
LEXAN™ PC Resin HF1140R
LEXAN™ PC Resin HF1140
LEXAN™ PC Resin HF1130R
LEXAN™ PC Resin HF1130
LEXAN™ PC Resin HF1110R
LEXAN™ PC Resin HF1110
LEXAN™ PC Resin GLX143
LEXAN™ PC Resin EX9332T
LEXAN™ PC Resin EX8681T
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
LEXAN™ PC Resin EM3110
LEXAN™ PC Resin AVP TLL80CU
Advanced Manufacturing