SABIC Lexan HF3510R High Flow
LEXAN™ Resin HF3510R is a high-flow polycarbonate designed for precision molding in automotive applications. With excellent mold release and easy processing, this raw material HF3510R delivers consistent performance for complex parts like bezels—available exclusively in opaque colors.
- Character: 39 MFR, MVR of 34. Mold release.
Typical property data
Mechanical Properties
- Tensile Strength at Yield: 60 MPa
- Tensile Modulus: 2,100 MPa
- Flexural Strength: 90 MPa
- Flexural Modulus: 2,200 MPa
- Elongation at Break: 110%
Impact Properties
- Notched Izod Impact (23°C): 65 kJ/m²
- Unnotched Izod Impact (23°C): No Break
Thermal Properties
- Heat Deflection Temp (1.8 MPa): 125°C
- Vicat Softening Temperature: 145°C
Physical Properties
- Melt Volume Rate (MVR): 34 cm³/10 min (at 300°C/1.2 kg)
- Density: 1.20 g/cm³
- Mold Shrinkage: 0.5 – 0.7%
Flame Performance
- UL94 Rating (1.5 mm): V2
- UL94 Rating (3.0 mm): V0
Processing Guidelines
- Recommended Melt Temperature: 280 – 310°C
- Mold Temperature: 80 – 120°C
- Drying Conditions: 2 – 4 hours at 120°C
Features & Benefits

Related Lexan™ Polycarbonate
LEXAN™ PC Resin HF3510R
LEXAN™ PC Resin HFR1723
LEXAN™ PC Resin HF1840R
LEXAN™ PC Resin HF1140R
LEXAN™ PC Resin HF1140
LEXAN™ PC Resin HF1130R
LEXAN™ PC Resin HF1130
LEXAN™ PC Resin HF1110R
LEXAN™ PC Resin HF1110
LEXAN™ PC Resin GLX143
LEXAN™ PC Resin EX9332T
LEXAN™ PC Resin EX8681T
LEXAN™ PC Resin EX7681T
LEXAN™ PC Resin EX7631T
LEXAN™ PC Resin EX6681T
LEXAN™ PC Resin EX5681T
LEXAN™ PC Resin AVP ZLL19CU
LEXAN™ PC Resin AVP ZLL12CP
Advanced Manufacturing