LEXAN™ PC Resin HFR1723

LEXAN™ PC Resin Sabic Tianjin

SABIC Lexan HFR1723 UV Stabilized

LEXAN™ HFR1723 resin is a 25 MFR polycarbonate. UV stabilized. Mold release. UL94 V2 rated. Available in transparent, limited package types. Ideal for durable components in electrical, consumer, and industrial applications.

  • Character: 25 MFR, UV stabilized. Mold release. UL94 V2 rated.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Typical property data

Mechanical Properties

  • Tensile Strength: 60 MPa
  • Flexural Modulus: 2,200 MPa
  • Flexural Strength: 90 MPa
  • Tensile Elongation at Break: 110%

Impact Properties

  • Notched Izod Impact (23°C): 60 J/m
  • Unnotched Izod Impact (23°C): No Break

Thermal Properties

  • Heat Deflection Temperature (1.8 MPa): 125°C
  • Vicat Softening Temperature: 145°C
  • Coefficient of Linear Thermal Expansion: 6.5 x 10⁻⁵ /°C

Physical Properties

  • Melt Flow Rate (MFR): 25 g/10 min (300°C/1.2 kg)
  • Density: 1.20 g/cm³
  • Transparency: Available in transparent grades

Flame Performance

  • UL94 Flame Rating: V2 @ 1.5 mm and 3.0 mm
  • Glow Wire Ignition Temperature (GWIT): 750°C

Processing Guidelines

  • Recommended Processing Temperature: 280–310°C
  • Mold Temperature: 80–110°C
  • Drying Conditions: 120°C for 3–4 hours

Features & Benefits

Engineered for Molding Efficiency

The built-in mold release agent ensures easy part ejection and faster cycle times, reducing your production costs and increasing output.

Built-In Safety & Durability

With its UL94 V-2 rating and UV stabilization, LEXAN HFR1723 delivers reliable flame retardancy and resists yellowing, ideal for long-lasting electronic housings and outdoor fixtures.

High Clarity with Robust Performance

This resin combines 88% light transmission with high impact resistance and good thermal stability, perfect for transparent covers, lenses, and protective components that require both visibility and durability.

LEXAN™ PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top