Chimei WONDERLITE® PC-681U
Chimei WONDERLITE PC-681U Flame Retardant Low Temperature Impact Resistance CHIMEI WONDERLITE® PC-681U is a flame-retardant, non-halogenated polycarbonate resin engineered for demanding environments. With 1.5mm V-0 flammability certification, exceptional low-temperature impact resistance (-30°C), and UV stability (UL 746C f1), it’s ideal for electrical enclosures, outdoor components, and safety-critical applications. Key technical data (ISO) Download Application WONDERLITE®
Chimei WONDERLITE® PC-681U Read More »