Chimei Polylac® PA-757F ABS

Chimei Polylac ABS Resin PA-757F

Polylac® PA-757F Low Residual Monomer Food Use ABS

POLYLAC® PA-757F ABS resin is a food-safe, high-performance plastic perfect for kitchenware, toys, and household items. With low monomer residue (EU 10/2011 certified), it combines safety, strength, and easy processing for reliable, everyday products.

  • Character: Low monomer residue (EU 10/2011 Certification)
  • Application: Food containers, kettles, kitchenware, toys
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Food-Safe & Certified

PA-757F meets strict EU food safety standards, ideal for containers, kettles, and kids’ toys. No harmful chemicals—safe for direct food contact.

Tough & Heat-Resistant

Withstands boiling water (104°C Vicat temp) and daily wear. High impact strength (19 KJ/m²) keeps products durable, even in cold or rough use.

Easy Molding

Smooth melt flow (18 ml/10 min) ensures fast, consistent molding. Low shrinkage (0.4-0.7%) reduces waste and fits tight production schedules.

Chimei Polylac® PA-757F

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.

Chimei Polylac® PA-757F Application

Polylac® PA-757F Datasheet

Low Residual Monomer ABS POLYLAC® PA-757F
Product Description: Low residual monomer, Food application
PropertiesISO Test MethodTest ConditionUnitPA-757F
Melt Flow Index1133220℃×10KGml/10 min18
Mass Density118323  ℃g/cm31.05
Tensile Strength52750 mm/min, yieldMPa47
50 mm/min, breakMPa34
Tensile Elongation52750 mm/min%40
Flexural Strength1782 mm/minMPa76
Flexural Modulus1782 mm/minGPa2.2
Izod Impact Strength180/1A23℃, NotchedKJ/m219
-30℃, NotchedKJ/m29
Charpy Impact Strength17923℃, NotchedKJ/m221
-30℃, NotchedKJ/m210
Vicat Softening Temp.30650℃/hr;1KG104
50℃/hr;5KG100
Heat Distortion Temp.75/A1.8MPa, unannealed83
1.8MPa, annealed98
Coefficient of Linear Thermal Expansion113598.6 x 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.7
Symbol1043>ABS<
March 11, 2024

Polylac® PA-757F UL Product iQ

POLYLAC® PA-757F UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
3.0 mmPLC 3
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 0UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 1
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm85   °C
3.0 mm85   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm80   °C
3.0 mm80   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm85   °C
3.0 mm85   °C

Related Polylac® ABS Plastics

No post found!

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top