FCFC TAIRILITE® AC3710 PC

FCFC TAIRILITE AC3710

TAIRILITE® AC3710 PC Resin Self Extinguishing Grade

TAIRILITE AC3710 is a halogen-free, flame-retardant polycarbonate resin combining high flow efficiency and non-transparency. This self-extinguishing grade excels in thin-walled applications like electronics and energy storage, delivering UL94 V-0 compliance, rapid molding, and robust impact resistance—ideal for safety-critical, high-performance components.

  • Manufacturer: CHIMEI
  • Character: Halogen free, Flame retardant, High flow, Non-transparency
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flame Retardancy: UL94 V-0 (0.6–3 mm), V-1 (0.45 mm), 5VB (1.5–3 mm)
  • Melt Flow Index: 28 g/10 min (300°C, 1.2 kg)
  • Impact Strength: 685 J/m (Izod), 40 kJ/m² (Charpy)
  • Heat Resistance: 120°C Vicat Softening Point
  • Specific Gravity: 1.2 (lightweight yet robust)
  • Molding Shrinkage: 0.5–0.7% (dimensional stability)
  • Certifications: UL File E162823, IEC/ISO compliant

Self-Extinguishing Safety

Tairilite PC AC3710’s self-extinguishing grade eliminates halogen additives while achieving UL94 V-0 compliance (0.6–3mm thickness), ensuring fire-resistant housings for high-risk environments like battery casings and energy storage systems.

High Flow for Precision Molding

With a melt flow index of 28g/10min, this resin fills intricate, thin-walled molds effortlessly—perfect for compact 3C electronics (e.g., <1mm laptop battery covers) without compromising structural integrity.

Impact Resistance Under Stress

Boasting IZOD impact strength of 685 J/m and Charpy impact of 40 kJ/m², TAIRILITE AC3710 withstands drops, vibrations, and mechanical stress, ideal for rugged housings in appliances and industrial equipment.

TAIRILITE AC3710

Application

  • Thin-Walled Electronics Casings: Laptop battery housings, smartphone components, tablet frames.
  • Energy Storage & EV Components: Battery module housings, EV charging connectors, power distribution units.
  • Household Appliances: Power tool housings, kitchen appliance switches, air conditioner internal parts.
  • Industrial Control Systems: Circuit breaker casings, control panel covers, sensor housings.
TAIRILITE AC3710 Application

Tairilite® AC3710 Datasheet

Self Extinguishing Grade FCFC TAIRILITE® AC3710 Data Sheet
Product Description: Halogen free, Flame retardant, High flow, Non-transparency
PropertyUnitTest MethodTest ConditionModel AC3710
Melt Flow Indexg/10 minISO 1133300℃ × 1.2kg28
IZOD Impact StrengthJ/mISO 18023 ℃ 3.2mm685
Charpy Impact StrengthkJ/m²ISO 17923 ℃ 4mm40
Specific GravityISO 118323℃/23℃1.2
Tensile StrengthMpaISO 52723 ℃63
Flexural StrengthMpaISO 17823 ℃104
Flexural ModulusMpaISO 17823 ℃2350
Rockwell HardnessR-scaleISO 2039-223℃R-122
Vicat Softening PointISO 306VICAT(10N ℃)120
Heat Deflection TemperatureISO 75/AUnannealed 18.6 kg/cm² (1.8MPa)(3.2mm)0.45
Molding Shrinkage%ISO 25773.2mm0.5 ~ 0.7
CombustibilityUL-94File No. E162823v-0 0.6 ~ 3 mm
v-1 0.45 mm
5VB 1.5 ~ 3 mm

Tairilite® AC3710 UL Product iQ

TAIRILITE® AC3710 UL Product iQ
File Number: E162823Polycarbonate (PC) “TAIRILITE”, furnished as pellets
ColorMin Thk (mm)Flame ClassHWIHAIRTI ElecRTI ImpRTI Str
ALL0.45V-140808080
0.6V-040808080
0.8V-020808080
1.5V-0, 5VB20808080
3V-0, 5VB00808080
Comparative Tracking Index (CTI):2Inclined Plane Tracking (IPT):
Dielectric Strength (kV/mm):Volume Resistivity (10x ohm-cm):
High-Voltage Arc Tracking Rate (HVTR):4High Volt, Low Current Arc Resis (D495):6
Dimensional Stability (%):
IEC and ISO Test Methods
Test NameTest MethodUnits Class (color)Thk (mm)Value
FlammabilityIEC 60695-11-10, IEC 60695-11-200.45V-1 (ALL)
0.6V-0 (ALL)
0.8V-0 (ALL)
1.5V-0, 5VB (ALL)
3V-0, 5VB (ALL)
Glow-Wire Flammability (GWFI)IEC 60695-2-12CC
Glow-Wire Ignition (GWIT)IEC 60695-2-13CC
IEC Comparative Tracking IndexIEC 60112Volts (Max)Volts (Max)
IEC Ball PressureIEC 60695-10-2CC
ISO Heat Deflection (1.80 MPa)ISO 75-2CC
ISO Tensile StrengthISO 527-2MPaMPa
ISO Flexural StrengthISO 178MPaMPa
ISO Tensile ImpactISO 8256kJ/m2kJ/m2
ISO Izod ImpactISO 180kJ/m2kJ/m2
ISO Charpy ImpactISO 179-2kJ/m2kJ/m2

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top