Covestro Makrolon® 9425 PC Resin
Makrolon 9425 Polycarbonate Granules 20% glass fiber reinforced Makrolon® 9425 by Covestro is a 20% glass fiber-reinforced, flame-retardant polycarbonate resin. With UL 94 V-0 (1.5mm) and 5VA (3.0mm) ratings, high viscosity, and easy-release properties, it excels in extrusion and injection molding. Ideal for opaque, high-safety industrial parts. Key technical data Mechanical Properties Thermal Performance Electrical
Covestro Makrolon® 9425 PC Resin Read More »