FIPC Formosa TARFLON™ A2200

FIPC Tarflon A2200

TARFLON™ A2200 Natural Color Injection Molding

Tarflon A2200 is a high-performance polycarbonate resin designed for injection molding and compounding. Combining exceptional impact resistance, thermal stability, and electrical insulation, it’s ideal for automotive, electronics, and industrial components. With natural color versatility and UL-certified safety, Tarflon A2200 delivers reliability in demanding environments while streamlining production efficiency.

  • Manufacturer: Formosa Idemitsu Petrochemical Corporation (FIPC)
  • Character: Basic PC with natural color for injection molding or compounding.
  • Application: for automotive, electronics, and industrial components
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Rate: 11 g/10min
  • Tensile Strength: 65 MPa
  • UL Flammability Rating: V-2 (0.36–2.9mm), HB (3.0–6.0mm)
  • Molding Parameters Pre-dry: at 120°C for 5–8 hours
  • Molding Parameters process: at 260–300°C
  • Optical Clarity: 85–90% light transmission

Unmatched Impact Resistance

With a Charpy impact strength of 80 kJ/m², Tarflon A2200 withstands high-stress environments, reducing part failure in automotive bumpers or protective equipment.

Heat-Resistant Durability

A heat deflection temperature of 125°C ensures stability in high-temperature applications like electronic housings or under-the-hood automotive components.

Superior Electrical Safety

Dielectric strength (30 kV/mm) and volume resistivity (>10¹⁶ Ω·cm) make it perfect for circuit breakers, connectors, and UL-rated industrial controls.

FIPC Tarflon PC resin

Application

  • Injection molded parts requiring high clarity and strength
  • Compounded materials for custom formulations
  • Transparent housings for consumer electronics
  • Automotive interior or lighting components
  • Medical device casings and enclosures
  • High-performance industrial equipment covers
Tarflon A2200 PC resin application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top