FIPC Formosa TARFLON™ IR1900

FIPC Tarflon IR1900

TARFLON™ IR1900 PC Resin General Grade High Transparency

Tarflon IR1900 is a premium iced-clear polycarbonate resin engineered for precision molding and extrusion. With NSF/ANSI 51 food safety certification, excellent mold release properties, and UL compliance, it’s ideal for electrical components, food-contact items, and safety equipment.

  • Manufacturer: Formosa Idemitsu Petrochemical Corporation (FIPC)
  • Character: General PC with iced-clear color and good mold release property
  • Application: for injection molding or extrusion
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Molding Efficiency: Low viscosity (MFR 19 g/10min)
  • Thermal Stability: Heat deflection up to 125°C; mold shrinkage 0.5–0.7%.
  • Electrical Safety: Volume resistivity >10¹⁶ Ω·cm, dielectric strength 30 kV/mm.
  • Durability: Rockwell hardness R120/M50, flexural strength 90 MPa.
  • Certifications: UL 94 V-2/HB, NSF/ANSI 51, UV/water resistance (UL746C f2)

Crystal-Clear Transparency & Safety

Tarflon IR1900 offers 85–90% luminous transmittance, mimicking glass-like clarity while being shatterproof. Perfect for decorative lighting covers, dishes, and contact lens cases where aesthetics and food safety matter.

Unmatched Impact Resistance

With a Charpy impact strength of 70 kJ/m²—the highest among plastics—Tarflon IR1900 withstands harsh drops and shocks. Ideal for relay cases, explosion-proof gloves, and safety lamps in rugged industrial settings.

UL-Certified Performance

UL94 V-2/HB flammability ratings and 130°C RTI ensure reliability in high-heat electrical equipment. Paired with NSF food compliance, it’s trusted for timer cases, cups, and electrical housings requiring strict safety standards.

FIPC Tarflon PC resin

Application

  • Electrical: Relay cases, timer cases, electrical housings.
  • Consumer Goods: Decorative lighting covers, cups, dishes, contact lens cases.
  • Safety Equipment: Explosion-proof gloves, safety lamps, industrial packs.
Tarflon IR1900 PC resin application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top