TARFLON™ IR2500 General Grade High Transparency
Tarflon IR2500 is a high-performance, iced-clear tarflon polycarbonate resin engineered for demanding applications. Combining 80 kJ/m² impact strength (highest among plastics), 85–90% light transmittance, and UL-certified flame resistance, it excels in extreme temperatures (-40°C to 125°C) while ensuring precision for injection molding and extrusion. Ideal for automotive, electronics, and NSF-certified food containers.
- Manufacturer: Formosa Idemitsu Petrochemical Corporation (FIPC)
- Character: General PC with iced-clear color and good mold release property.
- Application: for injection molding or extrusion
Key technical data (ISO)
- Flow Rate (MFR): 7 g/10min
- Impact Strength: 80 kJ/m²
- Heat Resistance: 125°C HDT
- Transparency: 85–90% light transmission
- Electrical Safety: UL94 V-2/HB flame rating + CTI PLC 2
- Food Safe: NSF/ANSI 51 certified
Download

Application
- Automotive: Headlamp covers, visors, and vibration-resistant components.
- Consumer Goods: Shatterproof cups, dishes, and decorative lighting.
- Electronics: Relay/timer cases, explosion-proof gloves, and equipment housings.
- Healthcare: Contact lens cases, safety goggles, and UV-resistant optics.
- Industrial: Electrical insulation parts, machinery housings, and outdoor safety gear.

Related TARFLON™ PC Plastics
FIPC Formosa TARFLON™ LC1500
FIPC Formosa TARFLON™ MD1500
FIPC Formosa TARFLON™ VT2500
FIPC Formosa TARFLON™ IV2500
FIPC Formosa TARFLON™ IV2200R
FIPC Formosa TARFLON™ IV1900R
FIPC Formosa TARFLON™ IR2500
FIPC Formosa TARFLON™ IR2200
FIPC Formosa TARFLON™ IR1900
FIPC Formosa TARFLON™ IR1700
FIPC Formosa TARFLON™ HQ2200
FIPC Formosa TARFLON™ A2200
FIPC Formosa TARFLON™ A1900
Advanced Manufacturing